StarRov 853 roving is designed for reinforcement in structural engineered thermoplastics.
StarRov 853 roving is designed for reinforcement in structural engineered thermoplastics.

Johns Manville (JM), which makes continuous filament glass fiber says that its StarRov 853 roving is available in both North America (225 Yield) and Europe (1200 and 2400 Tex).

StarRov 853 roving is designed for reinforcement in structural engineered thermoplastics, such as tapes and long-fiber thermoplastics (LFT) where high heat performance is required.

‘JM’s continuous innovation and product expansion globally for structural engineered thermoplastics is the result of great collaboration between our customers and our global product teams,’ said Karin Demez, global marketing and portfolio leader.

This story is reprinted from material from Johns Manvillewith editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.