3A Composites Core Materials has developed two new products in its Baltek range.

The company says that Baltek SealX can reduce resin uptake by more than 80% for rigid panels and 50% for flexible panels. SealX has been externally tested and approved by DNV-GL confirming resin savings.  

Baltek Adaptive ContourKore is a balsa finishing option which can help improve resin uptake and drapeability, thus reducing resin uptake further.

‘Our aim is to create green products that help our customers to become more efficient and positively impact the environment,’ said Eric Gauthier, CEO of 3A Composites Core Materials.