DSM has introduced a range of ultra-high-molecular-weight polyethylene (UHMWPE) material.

According to the company, its Trosar range is suitable for the hard and soft ballistic unidirectional laminate (UD), rope, netting, and aquaculture industries.  It is available in various performance grades including fiber and UD.

This story uses material from DSM, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.