Recent advances in computational materials science present novel opportunities for structure discovery and optimization, including uncovering of unsuspected compounds and metastable structures, electronic structure, surface, and nano-particle properties. The practical realization of these opportunities requires systematic generation and classification of the relevant computational data by high-throughput methods. In this paper we present Aflow (Automatic Flow), a software framework for high-throughput calculation of crystal structure properties of alloys, intermetallics and inorganic compounds. The Aflow software is available for the scientific community on the website of the materials research consortium, aflowlib.org. Its geometric and electronic structure analysis and manipulation tools are additionally available for online operation at the same website. The combination of automatic methods and user online interfaces provide a powerful tool for efficient quantum computational materials discovery and characterization.

This article originally appeared in Computational Materials Science 58, 2012, Pages 218–226.

Sign up or log in to your free Materials Today account to download the full article.

 

Already a Materials Today member?

Log in to your Materials Today account to access this feature.