A 'high quality' 3D-printed bioscaffold as designed with help from a machine learning algorithm developed at Rice University. Scale bar equals 1 millimeter. Image: Mikos Research Group/Rice University.A dose of artificial intelligence can speed the development of 3D-printed bioscaffolds that help injuries heal, according to researchers at Rice University.
A team led by computer scientist Lydia Kavraki of Rice's Brown School of Engineering used a machine learning approach to predict the quality of scaffold materials, given the printing parameters. The work also found that controlling print speed is critical in making high-quality implants.
Bioscaffolds developed by co-author and Rice bioengineer Antonios Mikos are bone-like structures that serve as placeholders for injured tissue. They are porous to support the growth of cells and blood vessels that turn into new tissue and ultimately replace the implant.
Mikos has been developing bioscaffolds, largely in concert with the Center for Engineering Complex Tissues, to improve techniques to heal craniofacial and musculoskeletal wounds. That work has progressed to include sophisticated 3D printing that can make a biocompatible implant custom-fit to the site of a wound.
That doesn't mean there isn't room for improvement. Machine learning techniques could help in designing materials and developing processes to create implants, speeding things up and eliminating much trial and error.
"We were able to give feedback on which parameters are most likely to affect the quality of printing, so when they continue their experimentation, they can focus on some parameters and ignore the others," said Kavraki, a renowned authority on robotics, artificial intelligence and biomedicine and director of Rice's Ken Kennedy Institute. The team reports its results in a paper in Tissue Engineering Part A.
The study identified print speed as the most important of five metrics the team measured, the others in descending order of importance being material composition, pressure, layering and spacing.
Mikos and his students had already considered bringing machine learning into the mix. The COVID-19 pandemic created a unique opportunity to pursue the project. "This was a way to make great progress while many students and faculty were unable to get to the lab," Mikos said.
The researchers first took advantage of a mass of data from a 2016 study on printing scaffolds with biodegradable poly(propylene fumarate), and then figured out what more was needed to train the computer models. "The students had to figure out how to talk to each other, and once they did, it was amazing how quickly they progressed," Kavraki said.
From start to finish, the COVID-19 window let them assemble data, develop models and get the results published within seven months, record time for a process that can often take years.
The team explored two modeling approaches. One was a classification method that predicted whether a given set of parameters would produce a 'low' or 'high' quality scaffold. The other was a regression-based approach that approximated the values of print-quality metrics to come to a result. Kavraki said that both relied upon a 'classical supervised learning technique' called random forest that builds multiple 'decision trees' and 'merges' them together to get a more accurate and stable prediction.
Ultimately, the collaboration could lead to better ways to quickly print a customized jawbone, kneecap or bit of cartilage on demand. "A hugely important aspect is the potential to discover new things," Mikos said. "This line of research gives us not only the ability to optimize a system for which we have a number of variables – which is very important – but also the possibility to discover something totally new and unexpected. In my opinion, that's the real beauty of this work.
"It's a great example of convergence. We have a lot to learn from advances in computer science and artificial intelligence, and this study is a perfect example of how they will help us become more efficient."
"In the long run, labs should be able to understand which of their materials can give them different kinds of printed scaffolds, and in the very long run, even predict results for materials they have not tried," Kavraki said. "We don't have enough data to do that right now, but at some point we think we should be able to generate such models."
Kavraki noted that The Welch Institute, recently established at Rice to enhance the university's already stellar reputation for advanced materials science, has great potential to expand such collaborations.
"Artificial intelligence has a role to play in new materials, so what the institute offers should be of interest to people on this campus," she said. "There are so many problems at the intersection of materials science and computing, and the more people we can get to work on them, the better."
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.