In this illustration, hydrogen molecules (white) sit between sheet-like floors of graphene (gray) that are supported by boron nitride pillars (pink and blue). Researchers found that identical structures made wholly of boron nitride had unprecedented capacity for storing hydrogen. Image: Lei Tao/Rice University. Engineers at Rice University have zeroed in on the optimal architecture for storing hydrogen in ‘white graphene’ nanomaterials. This is a design like a Lilliputian skyscraper, with ‘floors’ of boron nitride sitting one atop another and held precisely 5.2 angstroms apart by boron nitride pillars. The engineers report their finding in a paper in Small .
"The motivation is to create an efficient material that can take up and hold a lot of hydrogen – both by volume and weight – and that can quickly and easily release that hydrogen when it's needed," said the study's lead author, Rouzbeh Shahsavari, assistant professor of civil and environmental engineering at Rice.
Hydrogen is the lightest and most abundant element in the universe, and its energy-to-mass ratio – the amount of available energy per pound of raw material – far exceeds that of fossil fuels. It also offers the cleanest way to generate electricity, with water as the only by-product. A 2017 report by market analysts at BCC Research found that global demand for hydrogen storage materials and technologies will likely reach $5.4 billion annually by 2021.
Hydrogen's primary drawbacks relate to portability, storage and safety. While large volumes can be stored under high pressure in underground salt domes and specially designed tanks, small-scale portable tanks – the equivalent of an automobile gas tank – have so far eluded engineers.
Following months of calculations on two of Rice's fastest supercomputers, Shahsavari and Rice graduate student Shuo Zhao have now found the optimal architecture for storing hydrogen in boron nitride. One form of the material, hexagonal boron nitride (hBN), consists of atom-thick sheets of boron and nitrogen, and is sometimes called white graphene because the atoms are spaced exactly like carbon atoms in flat sheets of graphene.
Previous work in Shahsavari's Multiscale Materials Lab found that hybrid materials of graphene and boron nitride could hold enough hydrogen to meet the US Department of Energy (DOE)'s storage targets for light-duty fuel cell vehicles.
"The choice of material is important," he said. "Boron nitride has been shown to be better in terms of hydrogen absorption than pure graphene, carbon nanotubes or hybrids of graphene and boron nitride.
"But the spacing and arrangement of hBN sheets and pillars is also critical. So we decided to perform an exhaustive search of all the possible geometries of hBN to see which worked best. We also expanded the calculations to include various temperatures, pressures and dopants, trace elements that can be added to the boron nitride to enhance its hydrogen storage capacity."
Zhao and Shahsavari set up numerous ‘ab initio’ tests, computer simulations that used first principles of physics. Shahsavari said the approach was computationally intense but worth the extra effort because it offered the most precision.
"We conducted nearly 4000 ab initio calculations to try and find that sweet spot where the material and geometry go hand in hand and really work together to optimize hydrogen storage," he said.
Unlike materials that store hydrogen through chemical bonding, boron nitride is a sorbent that holds hydrogen through physical bonds, which are weaker than chemical bonds. But that's an advantage when it comes to getting hydrogen out of storage because sorbent materials tend to discharge more easily than their chemical cousins.
According to Shahsavari, the choice of boron nitride sheets or tubes and the corresponding spacing between them in the superstructure were the key to maximizing capacity.
"Without pillars, the sheets sit naturally one atop the other about 3 angstroms apart, and very few hydrogen atoms can penetrate that space," he said. "When the distance grew to 6 angstroms or more, the capacity also fell off. At 5.2 angstroms, there is a cooperative attraction from both the ceiling and floor, and the hydrogen tends to clump in the middle. Conversely, models made of purely BN tubes – not sheets – had less storage capacity."
Models showed that the pure hBN tube-sheet structures could hold 8 weight percent of hydrogen (weight percent is a measure of concentration, similar to parts per million). Physical experiments are needed to verify that capacity, but the DOE's ultimate target is 7.5 weight percent, and Shahsavari's models suggests that even more hydrogen can be stored in his structure if trace amounts of lithium are added to the hBN.
Finally, irregularities in the flat, floor-like sheets of the structure could also prove useful for engineers.
"Wrinkles form naturally in the sheets of pillared boron nitride because of the nature of the junctions between the columns and floors," he said. "In fact, this could also be advantageous because the wrinkles can provide toughness. If the material is placed under load or impact, that buckled shape can unbuckle easily without breaking. This could add to the material's safety, which is a big concern in hydrogen storage devices.
"Furthermore, the high thermal conductivity and flexibility of BN may provide additional opportunities to control the adsorption and release kinetics on-demand. For example, it may be possible to control release kinetics by applying an external voltage, heat or an electric field."
This story is adapted from material from Rice University , with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source .