Rice University researchers (from left) Ksenia Bets, Boris Yakobson and Nitant Gupta have simulated the growth of 2D monocrystals of hexagonal boron nitride and detailed the mechanism by which large crystals form on a stepped surface. Photo: Jeff Fitlow/Rice University.Very small steps make a big difference to researchers who want to create large wafers of two-dimensional (2D) materials. Atom-sized steps in a substrate provide the means for 2D crystals growing in a chemical vapor furnace to come together in perfect rank. Scientists have recently observed this phenomenon, and now a Rice University group has an idea why it works.
Rice materials theorist Boris Yakobson and researcher Ksenia Bets led the construction of simulations showing that atom-sized steps on a growth surface, or substrate, have the remarkable ability to keep monolayer crystal islands in alignment as they grow.
If the conditions are right, the islands join into a larger crystal without the grain boundaries that are so characteristic of 2D materials like graphene grown via chemical vapor deposition (CVD). That preserves their electronic perfection and characteristics, which differ depending on the material. The Rice scientists present their theory in a paper in Nano Letters.
Their investigation focused on hexagonal boron nitride (h-BN), aka white graphene, a crystal often grown via CVD. In this process, crystals nucleate at various places on a perfectly flat substrate material and not necessarily in alignment with each other.
However, recent experiments have demonstrated that growth on vicinal substrates – surfaces that appear flat but actually have sparse, atomically small steps – can align the crystals and help them merge into a single, uniform structure, as reported on arXiv. A co-author of that report and leader of the Korean team, Feng Ding, is an alumnus of the Yakobson lab and a current adjunct professor at Rice University.
But the experimentalists do not show how it works, as, Yakobson said, the steps are known to meander and be somewhat misaligned.
"I like to compare the mechanism to a 'digital filter,' here offered by the discrete nature of atomic lattices," he said. "The analog curve that, with its slopes, describes a meandering step is 'sampled and digitized' by the very grid of constituent atomic rows, breaking the curve into straight 1D-terrace segments. The slope doesn't help, but it doesn't hurt. Surprisingly, the match can be good; like a well-designed house on a hill, it stands straight.
"The theory is simple, though it took a lot of hard work to calculate and confirm the complementarity matching between the metal template and the h-BN, almost like for A-G-T-C pairs in strands of DNA."
It was unclear why the crystals merged into one so well until simulations by Bets, with the help of co-author and Rice graduate student Nitant Gupta, showed how the h-BN ‘islands’ remain aligned while nucleating along visibly curved steps.
"A vicinal surface has steps that are slightly misaligned within the flat area," Bets explained. "It has large terraces, but on occasion there will be one-atom-high steps. The trick by the experimentalists was to align these vicinal steps in one direction."
In CVD, a hot gas containing the atoms that will form the material is flowed into a chamber, where the atoms settle on the substrate and nucleate crystals. On a vicinal surface, the boron and nitrogen atoms prefer to settle in the crook of the steps.
"They have this nice corner where the atoms will have more neighbors, which makes them happier," Bets said. "They try to align to the steps and grow from there.
"But from a physics point of view, it's impossible to have a perfect, atomically flat step. Sooner or later, there will be small indentations, or kinks. We found that at the atomic scale, these kinks in the steps don't prevent h-BN from aligning if their dimensions are complementary to the h-BN structure. In fact, they help to ensure co-orientation of the islands."
Because the steps modeled by the Rice lab are just 1.27 angstroms deep, the growing crystals have little trouble surmounting the boundary. "Those steps are smaller than the bond distance between the atoms," Bets said. "If they were larger, like two angstroms or higher, it would be more of a natural barrier, so the parameters have to be adjusted carefully."
Two growing islands that approach each other zip together seamlessly, according to the simulations. Similarly, cracks that appear along steps easily heal, because the bonds between the atoms are strong enough to overcome the small distance.
Any path toward large-scale growth of 2D materials is worth pursuing for an army of applications, according to the researchers. Two-dimensional materials like conductive graphene, insulating h-BN and semiconducting transition metal dichalcogenides are the focus of intense scrutiny by researchers around the world. The Rice researchers hope their theoretical models will point the way toward growing large crystals of many kinds.
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.