Crystalline CHANGE TOPIC

Crystalline materials news, March 2017

Specially selected papers from Applied Materials Today

To celebrate the latest CiteScoreTracker value of 5.57, the Editor-in-Chief highlights three key articles.

A new a double perovskite nanofiber can be used as a highly efficient catalyst for oxygen evolution reactions in energy storage systems.

Water-based, biocompatible ink formulations of two-dimensional materials including graphene, MoS2, WS2, and hexagonal boron nitride.

Perovskite materials have optoelectronic properties promising for cheap, easy to make LEDs.

Metals with a gradient in grain size show increased overall strength while allowing ductile behavior to take place to avoid catastrophic failure.

Scientists have discovered that "layer-edge-states" are responsible for the high efficiencies seen with 2D layered hybrid perovskites.

Nanocrystalline doped ceramic oxide with zero-energy grain boundaries is as stable as bulk material.

Scientists have shown that DNA can control the assembly of bipyramidal gold nanoparticles into a complex crystal structure known as a clathrate.

The deadline is Monday 13 March 2017.

Colloidal spheres can self-assemble into diamond and pyrochlore crystal structures that form the basis for photonic crystals.

The deadline is Monday 13 March 2017.

A new method for healing low-quality diamond nanocrystals under high-temperature conditions could lead to their use in quantum sensing.

News archive…

Connect with us
Most viewed in crystalline materials…
News
 

A 3D model created by AI helped researchers to understand the formation of dislocations in complex polycrystalline materials.

Current research
 

Review
 

Feature
 

Read Yury Gogotsi's responses to his webinar: MXenes: a new family of two-dimensional materials.