Researchers have developed a specialized type of LMOF (molecular structure at center) that is designed to detect and remove heavy metal toxins from water. At upper left, mercury (HG2+) is taken in by the LMOF, while the graph at lower left shows how the LMOF's fluorescence is turned off as it binds with mercury. Images: Rutgers University. Tiny, glowing crystals designed to detect and capture heavy-metal toxins such as lead and mercury could prove to be a powerful new tool in locating and cleaning up contaminated water sources.
Motivated by the recent discoveries of high levels of heavy metals in drinking water in Flint, Michigan, and Newark, New Jersey, a science team led by researchers at Rutgers University used intense X-rays to probe the structure of the crystals they developed and learn how they bind heavy metals.
The crystals are known as luminescent metal-organic frameworks (LMOFs) and function like miniature, reusable sensors and traps. One type of LMOF that the team tested was found to selectively take up more than 99% of mercury from a test mixture of heavy and light metals within 30 minutes, according to recent results published in ACS Applied Materials and Interfaces . No other MOFs have performed as well in this dual role of detecting and capturing, or ‘adsorbing’, toxic heavy metals, the team reported.
Simon Teat, a staff scientist at Lawrence Berkeley National Laboratory (Berkeley Lab), studied individual LMOF crystals, each measuring about 100µm in size, with X-rays at the lab's Advanced Light Source (ALS). Using diffraction patterns produced as the X-ray light struck the LMOF samples, Teat applied software tools to map their three-dimensional structure with atomic resolution. The ALS is one of just a few synchrotron X-ray light sources in the world to have dedicated experimental stations for conducting chemical crystallography of crystallized chemical compounds such as MOFs.
Teat uncovered a patterned, grid-like three-dimensional (3D) structure containing carbon, hydrogen, oxygen, nitrogen and zinc atoms framing large, open channels. These atomic-scale structural details are key to understanding how the LMOFs bind heavy metals, and can also aid in designing more highly specialized structures.
"With MOFs, you're typically interested in using the holes for something," Teat explained. In this case, the structure allows heavy metals to enter these open channels and chemically bind to the MOFs. With a very open framework, the MOFs possess an abundant surface area relative to their size, allowing them to take in a large amount of contaminants.
The LMOF structure was engineered to glow by incorporating a fluorescent chemical component, or ligand. “When the metal (in the original structure of the MOF) binds to the fluorescent ligand, the resulting framework fluoresces,” Teat said. This fluorescence switches off when the LMOFs interact with the heavy metals.
According to Jing Li, a chemistry professor at Rutgers University who led the research, the technology could be a money-saving solution. "Others had developed MOFs for either the detection of heavy metals or for their removal, but nobody before had really investigated one that does both," Li added.
Intense X-rays produced at synchrotrons are the best way to map the 3D structure of the MOFs, Li said. "Knowing the crystal structures is one of the most important aspects of our research. You need those in order to perform subsequent characterizations and to understand the properties of these materials."
In their tests, the researchers found that the LMOFs would bind strongly to mercury and lead but weakly to lighter metals such as magnesium and calcium that are also found in water supplies but do not pose the same hazards. This selective trait, based on the molecular makeup of the LMOFs, is important, Li said. "We need to have a MOF that is selective and will only take the harmful species."
These LMOFs can also be recycled. The researchers found they could collect, clean, and then reuse the LMOFs for three cycles of toxic cleansing before their performance began to degrade.
Heavily industrialized areas, cities with antiquated water regulations and agricultural communities can be particularly susceptible to groundwater contamination, which can lead to soil contamination if not addressed. This can cause the contaminants to be taken up by plants and animals in the surrounding environment, broadening the pathways of exposure.
According to Li, further research could explore lower-cost and more durable LMOFs that last for more cycles, and researchers could also pursue the development of water filters by blending the LMOFs with polymers to create a solid film. "These filters could be used for capture on a larger scale," she suggested.
"We would like to continue with this research," Li said, adding that her team would like to test the system's performance on actual contaminated water sources if funding becomes available. "These are promising results, but we have a long way to go."
This story is adapted from material from Lawrence Berkeley National Laboratory , with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source .