The hardest substance in the human body is moved by its strongest muscles: When we heartily bite into an apple or a schnitzel, enormous strengths are working on the surface of our teeth. "What the natural tooth enamel has to endure also goes for dentures, inlays or bridges", glass chemist Prof. Dr. Dr. Christian Rüssel says. After all, these are worn as much as healthy teeth. Ceramic materials used so far are not very suitable for bridges, as their strengths are mostly not high enough. Now Prof. Rüssel and his colleagues of the Otto-Schott-Institute for Glass Chemistry succeeded in producing a new kind of glass-ceramic with a nanocrystalline structure, which seems to be well suited to be used in dentistry due to their high strength and its optical characteristics. The glass chemists of Jena University recently published their research results in the online-edition of the Journal of Biomedical Materials Research.
 
Glass-ceramics on the basis of magnesium-, aluminum-, and silicon oxide are distinguished by their enormous strength. "We achieve a strength five times higher than with comparable denture ceramics available today", Prof. Rüssel explains. The Jena glass chemists have been working for a while on high density ceramics, but so far only for utilization in other fields, for instance as the basis of new efficient computer hard drives. "In combination with new optical characteristics an additional field of application is opening up for these materials in dentistry", Prof. Rüssel is convinced.
 
Materials, to be considered as dentures are not supposed to be optically different from natural teeth. At the same time not only the right colour shade is important. "The enamel is partly translucent, which the ceramic is also supposed to be", Prof. Rüssel says.
 
To achieve these characteristics, the glass-ceramics are produced according to an exactly specified temperature scheme: First of all the basic materials are melted at about 1.500 °C, then cooled down and finely cut up. Then the glass is melted again and cooled down again. Finally, nanocrystals are generated by controlled heating to about 1,000 °C. "This procedure determines the crystallization crucial for the strength of the product", the glass chemist Rüssel explains. But this was a technical tightrope walk. Because a too strongly crystallized material disperses the light, becomes opaque and looks like plaster. The secret of the Jena glass ceramic lies in its consistence of nanocrystals. The size of these is at most 100 nanometers in general. "They are too small to strongly disperse light and therefore the ceramic looks translucent, like a natural tooth", Prof. Rüssel says.
 
A lot of developing work is necessary until the materials from the Jena Otto-Schott-Institute will be able to be used as dentures. But the groundwork is done. Prof. Rüssel is sure of it.
 
This story is reprinted from material from the Friedrich Schiller University Jena, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.