Scientists at the University of Chicago have developed a new technique to 'sew' two patches of crystals seamlessly together at the atomic level to create atomically-thin fabrics. Image: Park et al. Joining different kinds of materials together can lead to all kinds of breakthroughs. It's an essential skill that allowed humans to make everything from skyscrapers (by reinforcing concrete with steel) to solar cells (by layering materials to herd electrons).
In electronics, joining different materials together produces heterojunctions, which are fundamental components in solar cells, LEDs and computer chips. The smoother the seam between the two materials, the more easily electrons flow across it, making them essential for determining how well the electronic devices function. What make this tricky is that the two materials are crystals, rigid lattices of atoms that may have very different spacings and don't take kindly to being mashed together.
In a paper in Science , scientists at the University of Chicago and Cornell University report a new technique for ‘sewing’ two patches of crystals seamlessly together at the atomic level to create atomically-thin fabrics.
The team wanted to do this by stitching together different fabric-like, three-atom-thick crystals. "Usually, these are grown in stages under very different conditions: grow one material first, stop the growth, change the condition and start it again to grow another material," explained Jiwoong Park, professor of chemistry in the James Franck Institute and the Institute for Molecular Engineering at the University of Chicago and a lead author of the paper.
Instead, the scientists developed a new process for finding the perfect window that would work for both materials in a constant environment, so they could grow the entire crystal in a single session. According to Park, the resulting single-layer materials are the most perfectly aligned ever grown. The gentler transition meant that, at the points where the two lattices meet, one lattice stretches or grows to meet the other, instead of leaving holes or other defects. The atomic seams are so tight, in fact, that when the scientists looked up close with scanning electron microscopes, they saw that the larger of the two materials puckers a little around the joint.
They decided to test the performance of this heterojunction in one of the most widely used electronic devices: a diode. When two different materials are joined, the electrons are supposed to be able to flow one way through the ‘fabric’, but not the other.
The diode lit up. "It was exciting to see these three-atom-thick LEDs glowing. We saw excellent performance – the best known for these types of materials," said Saien Xie, a graduate student and first author of the paper.
This discovery opens up some interesting ideas for electronics. Devices like LEDs are currently stacked in layers and are usually on a rigid surface. But Park said the new technique could open up new configurations, like flexible LEDs or atom-thick 2D circuits that work both horizontally and laterally.
He also noted that the stretching and compressing changed the optical properties of the crystals due to quantum mechanical effects. This suggests potential for using these heterojunctions as light sensors and LEDs that could be tuned to different colors, for example, or strain-sensing fabrics that change color as they're stretched.
"This is so unknown that we don't even know all the possibilities it holds yet," Park said. "Even two years ago it would have been unimaginable."
This story is adapted from material from the University of Chicago , with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source .