Skyrmions, subatomic quasiparticles that could play a key role in future spintronic technologies, have been observed for the first time using x-rays. An international collaboration of researchers working at Berkeley Lab’s Advanced Light Source (ALS) observed skyrmions in copper selenite (Cu2SeO3) an insulator with multiferroic properties. The results not only hold promise for ultracompact data storage and processing, but may also open up entire new areas of study in the emerging field of quantum topology.
“Using resonant x-ray scattering, we were able to gather unique element-specific, orbital-sensitive electronic and magnetic structural information not available by any other method,” says Sujoy Roy, a physicist who oversees research at ALS Beamline 12.0.2 where the study was carried out.
“We found the unexpected existence of two distinct skyrmion sub-lattices that rotate with respect to each other, creating a moiré-like pattern,” Roy says. “Compared to materials with a simpler magnetic structure, the sub-lattices provide for an extra degree of freedom to minimize the free energy. This leads to magnetic excitations that can’t exist in materials with a single magnetic lattice structure.”
“We were able to show that although the skyrmions act like magnetic particles, their origin in copper selenite is electronic...”Matthew Langner, lead author.
Although skyrmions act like baryons, they are actually magnetic vortices – discrete swirls of magnetism – formed from the spins of charged particles. Spin is a quantum property in which the charged particles act as if they were bar magnets rotating about an axis and pointing in either an “up” or “down” direction. The discovery of skyrmions – named for Tony Skyrme, a British physicist who first theorized their existence – in manganese silicide generated much excitement in the materials sciences world because their exotic hedgehog-like spin texture is topologically protected – meaning it can’t be perturbed. Add to this the discovery that skyrmions can be moved coherently over macroscopic distances with a tiny electrical current and you have a strong spintronic candidate.
“A major breakthrough came with the discovery of skyrmions in copper selenite because its magnetic properties can be controlled with an electric field,” says Roy. “To achieve this control, however, we must understand how different electron orbitals stabilize the skyrmionic phase. Until our study, the copper selenite skyrmions had only been observed with neutron scattering and transmission electron microscopy, techniques that are insensitive to electron orbitals.”
ALS Beamline 12.0.2 is an undulator beamline with experimental facilities optimized for coherent x-ray scattering studies of magnetic materials. The collaboration, which included researchers from Berkeley Lab’s Materials Sciences Division and Japan’s RIKEN institute, used these facilities to first identify the magnetic vortex. Then, at a certain applied electric field and temperature, they saw x-ray signals due to the formation of a skyrmion lattice.
“We were able to show that although the skyrmions act like magnetic particles, their origin in copper selenite is electronic,” says Matthew Langner, lead author of the Physical Review Letters paper. “We also found that temperature can be used to move the skyrmions in copper selenite in either a clockwise or counter-clockwise direction.”
Controlling the movement of skyrmions in a multiferroic compound suggests these magnetic vortices could be used to read and write data. Skyrmions are considered especially promising for the holographic information storage concept known as magnetic race-track memory.
“The skyrmion is topologically distinct from the other ground-state magnetic structures, meaning it can be moved around the sample without losing its shape,” Langner says. “The combination of this stability and the low magnetic and electric fields required for manipulating the skyrmions is what makes them potentially useful for spintronic applications.”
In addition to device applications, the collaboration’s findings show that is now possible to use x-rays to study spectroscopic and electronic aspects of the skyrmion, and to study skyrmion dynamics on the time-scale of fundamental interactions.
This story is reprinted from material from Berkeley Lab, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.