Much like pulling blocks from a tower in a Jenga game, scientists used chemistry to neatly remove a layer of oxygen atoms from a perovskite material. This flipped the material into a new atomic structure – a nickelate – that can conduct electricity with 100% efficiency. Image: Greg Stewart/SLAC National Accelerator Laboratory.Scientists at the US Department of Energy's SLAC National Accelerator Laboratory and Stanford University have made the first nickel oxide material that shows clear signs of superconductivity – the ability to transmit electrical current without loss.
Also known as a nickelate, it's the first in a potential new family of unconventional superconductors that's very similar to the copper oxides, or cuprates. The discovery of cuprates in 1986 raised hopes that superconductors could someday operate at close to room temperature and revolutionize electronic devices, power transmission and other technologies. The similarities with cuprates have scientists wondering if this family of nickelates could also superconduct at relatively high temperatures.
At the same time, the new material seems different from the cuprates in fundamental ways – for instance, it may not contain a type of magnetism that all the superconducting cuprates have – and this could overturn leading theories of how these unconventional superconductors work. After more than three decades of research, no one has pinned that down.
The experiments were led by Danfeng Li, a postdoctoral researcher with the Stanford Institute for Materials and Energy Sciences at SLAC, and are reported in a paper in Nature.
"This is a very important discovery that requires us to rethink the details of the electronic structure and possible mechanisms of superconductivity in these materials," said George Sawatzky, a professor of physics and chemistry at the University of British Columbia in Canada, who was not involved in the study but wrote a commentary that accompanied the paper in Nature. "This is going to cause an awful lot of people to jump into investigating this new class of materials, and all sorts of experimental and theoretical work will be done."
Ever since the cuprate superconductors were discovered, scientists have dreamed of making similar oxide materials based on nickel, which is right next to copper on the periodic table of the elements. But making nickelates with an atomic structure that's conducive to superconductivity turned out to be unexpectedly hard.
"As far as we know, the nickelate we were trying to make is not stable at the very high temperatures – about 600°C – where these materials are normally grown," Li said. "So we needed to start out with something we can stably grow at high temperatures and then transform it at lower temperatures into the form we wanted."
He started with a perovskite – a material defined by its unique, double-pyramid atomic structure – made of neodymium, nickel and oxygen. Then he doped the perovskite by adding strontium – a common process that adds chemicals to a material to make more of its electrons flow freely.
This stole electrons away from the nickel atoms, leaving vacant ‘holes’, and the nickel atoms were not happy about it, Li said. The material was now unstable, making the next step – growing a thin film of the material on a surface – really challenging; it took him half a year to get it to work.
Once that was done, Li cut the film into tiny pieces, loosely wrapped it in aluminum foil and sealed it in a test tube with a chemical that neatly snatched away a layer of its oxygen atoms – much like removing a stick from a wobbly tower of Jenga blocks. This flipped the film into an entirely new atomic structure – a strontium-doped nickelate.
"Each of these steps had been demonstrated before," Li said, "but not in this combination."
Li remembers the exact moment in the laboratory, around 2 am, when tests indicated that the doped nickelate might be superconducting. He was so excited that he stayed up all night, and in the morning co-opted the regular meeting of his research group to show them what he'd found. Soon, many of the group members joined him in a round-the-clock effort to improve and study this material.
Further testing would reveal that the nickelate was indeed superconducting in a temperature range of 9–15K – incredibly cold, but a good start, with possibilities of higher temperatures ahead.
Research on the new material is at a ‘very, very early stage, and there's a lot of work ahead’, cautioned Harold Hwang, a professor at SLAC and Stanford, and senior author of the paper. "We have just seen the first basic experiments, and now we need to do the whole battery of investigations that are still going on with cuprates."
Among other things, he said, scientists will want to dope the nickelate material in various ways to see how this affects its superconductivity across a range of temperatures, and determine whether other nickelates can become superconducting. Other studies will explore the material's magnetic structure and its relationship to superconductivity.
This story is adapted from material from the SLAC National Accelerator Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.