Researchers have found a way to trigger the innate, but previously hidden, ability of graphene to act as a superconductor – meaning that it can be made to carry an electrical current with zero resistance.
The finding, reported in a paper in Nature Communications, further enhances the potential of graphene, which is already widely seen as a material that could revolutionize industries such as healthcare and electronics. Graphene is a two-dimensional sheet of carbon atoms that combines several remarkable properties: it is very strong, but also light and flexible, and highly conductive.
Since its discovery in 2004, scientists have speculated that graphene may also have the capacity to be a superconductor. Until now, superconductivity in graphene has only been achieved by doping it with, or by placing it on, a superconducting material – a process that can compromise some of its other properties.
But in the new study, researchers at the University of Cambridge in the UK managed to activate the dormant potential for graphene to superconduct in its own right. This was achieved by coupling it with a material called praseodymium cerium copper oxide (PCCO).
Superconductors are already used in numerous applications. Because they can generate large magnetic fields, they are an essential component in MRI scanners and levitating trains. They could also be used to make energy-efficient power lines and devices capable of storing energy for millions of years.
Superconducting graphene opens up yet more possibilities. The researchers suggest, for example, that graphene could now be used to create new types of superconducting quantum devices for high-speed computing. Intriguingly, it might also be used to prove the existence of a mysterious form of superconductivity known as ‘p-wave’ superconductivity, which academics have been struggling to verify for more than 20 years.
The research was led by Angelo Di Bernardo and Jason Robinson, Fellows at St John's College, University of Cambridge. Other members of their team included: Andrea Ferrari from the Cambridge Graphene Centre; Oded Millo from the Hebrew University of Jerusalem in Israel; and Jacob Linder at the Norwegian University of Science and Technology in Trondheim.
"It has long been postulated that, under the right conditions, graphene should undergo a superconducting transition, but can't. The idea of this experiment was, if we couple graphene to a superconductor, can we switch that intrinsic superconductivity on?"Jason Robinson, University of Cambridge
"It has long been postulated that, under the right conditions, graphene should undergo a superconducting transition, but can't," Robinson said. "The idea of this experiment was, if we couple graphene to a superconductor, can we switch that intrinsic superconductivity on? The question then becomes how do you know that the superconductivity you are seeing is coming from within the graphene itself, and not the underlying superconductor?"
Similar approaches have been taken in previous studies using metallic-based superconductors, but with limited success. "Placing graphene on a metal can dramatically alter the properties so it is technically no longer behaving as we would expect," Di Bernardo said. "What you see is not graphene's intrinsic superconductivity, but simply that of the underlying superconductor being passed on."
PCCO is an oxide from a wider class of superconducting materials called ‘cuprates’, which have well-understood electronic properties. This meant that, using a technique called scanning and tunneling microscopy, the researchers could distinguish the superconductivity in PCCO from the superconductivity observed in graphene.
Superconductivity is characterized by the way the electrons interact: within a superconductor, electrons form pairs, and the spin alignment between the electrons of a pair may be different depending on the type – or ‘symmetry’ – of superconductivity involved. In PCCO, for example, the pairs' spin state is misaligned (antiparallel), in what is known as a ‘d-wave state’.
By contrast, when graphene was coupled to superconducting PCCO in the Cambridge-led experiment, the results suggested that the electron pairs within graphene were in a p-wave state. "What we saw in the graphene was, in other words, a very different type of superconductivity than in PCCO," Robinson said. "This was a really important step because it meant that we knew the superconductivity was not coming from outside it and that the PCCO was therefore only required to unleash the intrinsic superconductivity of graphene."
It remains unclear what type of superconductivity the team activated, but their results strongly indicate that it is the elusive ‘p-wave’ form. If so, the study could transform the ongoing debate about whether this mysterious type of superconductivity exists, and – if so – what exactly it is.
In 1994, researchers in Japan fabricated a triplet superconductor that may have had p-wave symmetry, using a material called strontium ruthenate (SRO). The p-wave symmetry of SRO has never been fully verified, partly due to the fact that SRO is a bulky crystal, which makes it challenging to fabricate into the type of devices required to test theoretical predictions.
"If p-wave superconductivity is indeed being created in graphene, graphene could be used as a scaffold for the creation and exploration of a whole new spectrum of superconducting devices for fundamental and applied research areas," Robinson said. "Such experiments would necessarily lead to new science through a better understanding of p-wave superconductivity, and how it behaves in different devices and settings."
The study also has further implications. For example, it suggests that graphene could be used to make a transistor-like device in a superconducting circuit, and that its superconductivity could be incorporated into molecular electronics. "In principle, given the variety of chemical molecules that can bind to graphene's surface, this research can result in the development of molecular electronics devices with novel functionalities based on superconducting graphene," Di Bernardo added.
This story is adapted from material from St John's College, University of Cambridge, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.