For the first time, a group of chemists, physicists, and engineers has developed crystalline materials that allow an optical fiber to have integrated, high-speed electronic functions. The potential applications of such optical fibers include improved telecommunications and other hybrid optical and electronic technologies, improved laser technology, and more-accurate remote-sensing devices. The research was initiated by Rongrui He, a postdoctoral researcher in the Department of Chemistry at Penn State University. The international team, led by John Badding, a professor of chemistry at Penn State, will publish its findings in the journal Nature Photonics.
 
Badding explained that one of the greatest current technological challenges is exchanging information between optics and electronics rapidly and efficiently. Existing technology has resulted in sometimes-clumsy ways of merging optical fibers with electronic chips -- silicon-based integrated circuits that serve as the building blocks for most semiconductor electronic devices such as solar cells, light-emitting diodes (LEDs), computers, and cell phones. "The optical fiber is usually a passive medium that simply transports light, while the chip is the piece that performs the electrical part of the equation," Badding said. "For example, light is transmitted from London to New York via fiber-optic cables when two people set up a video call on their computers. But the computer screens and associated electronic devices have to take that light and convert it to an image, which is an electrical process. Light and electricity are working in concert in a process called an OEO conversion, or an optical-electrical-optical conversion." Badding said that, ideally, rather than coupling the optical fiber to the chip, as is routine in existing technology, a "smart fiber" would have the electronic functions already built in.
 
The integration of optical fibers and chips is difficult for many reasons. First, fibers are round and cylindrical, while chips are flat, so simply shaping the connection between the two is a challenge. Another challenge is the alignment of pieces that are so small. "An optical fiber is 10 times smaller than the width of a human hair. On top of that, there are light-guiding pathways that are built onto chips that are even smaller than the fibers by as much as 100 times," Badding said. "So imagine just trying to line those two devices up. That feat is a big challenge for today's technology."
 
To address these challenges, the team members took a different approach. Rather than merge a flat chip with a round optical fiber, they found a way to build a new kind of optical fiber with its own integrated electronic component, thereby bypassing the need to integrate fiber-optics onto a chip. To do this, they used high-pressure chemistry techniques to deposit semiconducting materials directly, layer by layer, into tiny holes in optical fibers. "The big breakthrough here is that we don't need the whole chip as part of the finished product. We have managed to build the junction -- the active boundary where all the electronic action takes place -- right into the fiber," said Pier J. A. Sazio of the University of Southampton in the United Kingdom and one of the team's leaders. "Moreover, while conventional chip fabrication requires multimillion-dollar clean-room facilities, our process can be performed with simple equipment that costs much less."
 
Sazio added that one of the key goals of research in this field is to create a fast, all-fiber network. "If the signal never leaves the fiber, then it is a faster, cheaper, and more efficient technology," said Sazio. "Moving technology off the chip and directly onto the fiber, which is the more-natural place for light, opens up the potential for embedded semiconductors to carry optoelectronic applications to the next level. At present, you still have electrical switching at both ends of the optical fiber. If we can actually generate signals inside a fiber, a whole range of optoelectronic applications becomes possible."
 
The research also has many potential non-telecommunications applications. "For example, our work also represents a very different approach to fabricating semiconductor junctions that we are investigating for solar-cell applications," said Badding.
 
This story is reprinted from material from Penn State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.