Tanvi Upreti, doctoral student in the Division for Complex Materials and Devices at Linköping University, who helped carry out the experiments on water traps in organic semiconductors. Photo: Charlotte Perhammar.Poor-quality organic semiconductors can become high-quality semiconductors when manufactured in the correct way. Researchers at Linköping University in Sweden report in a paper in Nature Materials that the motion of charges in organic electronic devices can be dramatically slowed by minute amounts of water.
The discovery that organic materials, such as polymers, can act as semiconductors led to a Nobel Prize in Chemistry in 2000. Since then, research within organic electronics has truly exploded, not least at Linköping University, which is home to world-leading research in the field.
Organic semiconductors, however, do not conduct current as efficiently as semiconductors made of silicon or other inorganic materials. Scientists have discovered that one of the causes of this is the formation of traps in the organic materials in which the charge carriers get stuck. Several research groups around the world have been working hard to understand not only where these traps are located, but how they can be eliminated.
"There are traps in all organic semiconductors, but they are probably a greater problem in n-type materials, since these are generally poorer semiconductors than p-type materials," says Martijn Kemerink, professor of applied physics in the Division for Complex Materials and Devices at Linköping University. Materials of p-type have a positive charge and their charge carriers consist of holes, while materials of n-type have charge carriers in the form of electrons, which give the material a negative charge.
Kemerink and his colleagues at Linköping University have concluded that water is the villain of the piece. Specifically, they think that water absorbed from the environment sits in nanometer-sized pores in the organic material.
"In a p-type material the dipoles in the water align with their negative ends towards the holes, which are positively charged, and the energy of the complete system is lowered. You could say that the dipoles embed the charge carriers such that they cannot go anywhere anymore" says Kemerink. For n-type materials, the water orients the other way around, but the effect is the same – the charge is trapped.
Experiments have been carried out in which organic semiconductors are heated to dry them out and evaporate the water. While this works fine for a while, the material just ends up re-absorbing water from the surrounding air, and so much of the benefit gained by drying disappears.
"The more water, the more traps," explains Kemerink. "We have also shown that the drier the films can be manufactured, the better conductors they are. The theoretical work by Mathieu Linares quantitatively confirmed our ideas about what was going on, which was very satisfactory. Our article in Nature Materials shows not only how to get the water out, but also how to make sure that the water stays out, in order to produce an organic material with stable conductivity."
In order to prevent the re-uptake of water into the material once it has been dried, the scientists developed a way to remove the voids into which the water molecules otherwise would have penetrated. Their method is based on heating the material in the presence of a suitable organic solvent.
"Materials that were previously believed to be extremely poor semiconductors can instead become good semiconductors, as long as they are manufactured in a dry atmosphere," says Kemerink. "We have shown that dry-prepared materials tend to remain dry, while materials that are made in the presence of water can be dried. The latter are, however, extremely sensitive to water. This is true of the materials we have tested, but there's nothing to suggest that other organic semiconducting materials behave differently."
This story is adapted from material from Linköping University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.