"The devices we're making are very much like cryotrons in that they don't require Josephson junctions."Karl Berggren, MIT
Superconductors – materials that conduct electricity without resistance – are remarkable. They provide a macroscopic glimpse into quantum phenomena, which are usually observable only at the atomic level. Beyond their physical peculiarity, superconductors are also useful. They're found in medical imaging, quantum computers and cameras used with telescopes.
But superconducting devices can be finicky. Often, they're expensive to manufacture and prone to errors from environmental noise. That could change, however, thanks to research from Karl Berggren's group in the Department of Electrical Engineering and Computer Science at Massachusetts Institute of Technology (MIT).
The researchers are developing a superconducting nanowire, which could lead to more efficient superconducting electronics. The nanowire's potential benefits derive from its simplicity, says Berggren. "At the end of the day, it's just a wire."
Berggren will present a summary of this research at the 2021 IEEE Solid-state Circuits Conference.
Most metals lose resistance and become superconducting at extremely low temperatures, usually just a few degrees above absolute zero. Superconductors are already used to sense magnetic fields, especially in highly sensitive situations like monitoring brain activity, and also have applications in both quantum and classical computing.
Underlying many of these superconductors is a device invented in the 1960s called the Josephson junction – essentially two superconductors separated by a thin insulator. "That's what led to conventional superconducting electronics, and then ultimately to the superconducting quantum computer," says Berggren.
However, the Josephson junction "is fundamentally quite a delicate object", Berggren adds. That translates directly into the cost and complexity of manufacturing, especially for the thin insulating layer.
Josephson junction-based superconductors also may not play well with others. "If you try to interface it with conventional electronics, like the kinds in our phones or computers, the noise from those just swamps the Josephson junction," Berggren explains. "So, this lack of ability to control larger-scale objects is a real disadvantage when you're trying to interact with the outside world."
To overcome these disadvantages, Berggren is developing a new technology – the superconducting nanowire – with roots older than the Josephson junction itself.
In 1956, MIT electrical engineer Dudley Buck published a description of a superconducting computer switch called the cryotron. This device was little more than two superconducting wires: one was straight and the other was coiled around it. The cryotron acts as a switch, because when current flows through the coiled wire, its magnetic field reduces the current flowing through the straight wire.
At the time, the cryotron was much smaller than other types of computing switches, like vacuum tubes or transistors, and Buck thought the cryotron could become the building block of computers. But in 1959, Buck died suddenly at age 32, halting the development of the cryotron. (Since then, transistors have been scaled down to microscopic sizes and today make up the core logic components of computers.)
Now, Berggren is rekindling Buck's ideas about superconducting computer switches. "The devices we're making are very much like cryotrons in that they don't require Josephson junctions," he says. He dubbed his superconducting nanowire device the nano-cryotron in tribute to Buck – though it works a bit differently to the original cryotron.
The nano-cryotron uses heat to trigger a switch, rather than a magnetic field. In Berggren's device, current runs through a superconducting, supercooled wire called the 'channel'. That channel is intersected by an even smaller wire called a 'choke' – like a multilane highway intersected by a side road. When current is sent through the choke, its superconductivity breaks down and it heats up. Once that heat spreads from the choke to the main channel, it causes the main channel to lose its superconducting state as well.
Berggren's group has already demonstrated proof-of-concept for the nano-cryotron's use as an electronic component. A former student of Berggren's, Adam McCaughan, developed a device that uses nano-cryotrons to add binary digits. And Berggren has successfully used nano-cryotrons as an interface between superconducting devices and classical, transistor-based electronics.
Berggren says his group's superconducting nanowire could one day complement – or perhaps compete with – Josephson junction-based superconducting devices. "Wires are relatively easy to make, so it may have some advantages in terms of manufacturability," he says.
He thinks the nano-cryotron could one day find a home in superconducting quantum computers and supercooled electronics for telescopes. Wires have low power dissipation, so they may also be handy for energy-hungry applications, he says. "It's probably not going to replace the transistors in your phone, but if it could replace the transistor in a server farm or data center? That would be a huge impact."
Beyond specific applications, Berggren takes a broad view of his work on superconducting nanowires. "We're doing fundamental research, here. While we're interested in applications, we're just also interested in: What are some different kinds of ways to do computing? As a society, we've really focused on semiconductors and transistors. But we want to know what else might be out there."
This story is adapted from material from MIT, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.