Using NERSC’s Cray XC30 supercomputer “Edison,” University of Michigan researchers Dylan Bayerl and Emmanouil Kioupakis found that the semiconductor indium nitride (InN), which typically emits infrared light, will emit green light if reduced to 1 nanometer-wide wires. Moreover, just by varying their sizes, these nanostructures could be tailored to emit different colors of light, which could lead to more natural-looking white lighting while avoiding some of the efficiency loss today’s LEDs experience at high power.
LEDs are semiconductor devices that emit light when an electrical current is applied. Today’s LEDs are created as multilayered microchips. The outer layers are doped with elements that create an abundance of electrons on one layer and too few on the other. The missing electrons are called holes. When the chip is energized, the electrons and holes are pushed together, confined to the intermediate quantum-well layer where they are attracted to combine, shedding their excess energy (ideally) by emitting a photon of light.
At low power, nitride-based LEDs (most commonly used in white lighting) are very efficient, converting most of their energy into light. But turn the power up to levels that could light up a room and efficiency plummets, meaning a smaller fraction of electricity gets converted to light. This effect is especially pronounced in green LEDs, giving rise to the term “green gap.”
Nanomaterials offer the tantalizing prospect of LEDs that can be “grown” in arrays of nanowires, dots or crystals. The resulting LEDs could not only be thin, flexible and high-resolution, but very efficient, as well.
The energy difference between an LED’s electrons and holes, called the bandgap, determines the wavelength of the emitted light. The wider the bandgap, the shorter the wavelength of light. The bandgap for bulk InN is quite narrow, only 0.6 electron volts (eV), so it produces infrared light. In Bayerl and Kioupakis’ simulated InN nanostructures, the calculated bandgap increased, leading to the prediction that green light would be produced with an energy of 2.3eV.
That bodes well for creating more natural-looking light from LEDs. By mixing red, green and blue LEDs engineers can fine tune white light to warmer, more pleasing hues. This “direct” method isn’t practical today because green LEDs are not as efficient as their blue and red counterparts. Instead, most white lighting today comes from blue LED light passed through a phosphor, a solution similar to fluorescent lighting and not a lot more efficient. Direct LED lights would not only be more efficient, but the color of light they produce could be dynamically tuned to suit the time of day or the task at hand.
Using pure InN, rather than layers of alloy nitride materials, would eliminate one factor that contributes to the inefficiency of green LEDs: nanoscale composition fluctuations in the alloys. These have been shown to significantly impact LED efficiency.
Also, using nanowires to make LEDs eliminates the “lattice mismatch” problem of layered devices. “When the two materials don’t have the same spacing between their atoms and you grow one over the other, it strains the structure, which moves the holes and electrons further apart, making them less likely to recombine and emit light,” said Kioupakis, who discovered this effect in previous research that also drew on NERSC resources. “In a nanowire made of a single material, you don’t have this mismatch and so you can get better efficiency,” he explained.
The researchers also suspect the nanowire’s strong quantum confinement contributes to efficiency by squeezing the holes and electrons closer together, a subject for future research. “Bringing the electrons and holes closer together in the nanostructure increases their mutual attraction and increases the probability that they will recombine and emit light.” Kioupakis said.
While this result points the way towards a promising avenue of exploration, the researchers emphasize that such small nanowires are difficult to synthesize. However, they suspect their findings can be generalized to other types of nanostructures, such as embedded InN nanocrystals, which have already been successfully synthesized in the few-nanometers range.
This story is reprinted from material from NERSC, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.