Economically competitive fusion
Volume 11, Issue 12, Page 46–53
| David J. Ward, Sergei L. Dudarev
Not since the oil crisis of the 1970s has the perception that energy is a crucial and precious resource been as strong as it is today. The need for a new approach to world energy supply, driven by concerns over resources, pollution, and security, is leading to a reappraisal of fusion. Fusion has enormous potential and major safety and environmental advantages, and hence could make a large difference to energy supplies.