Researchers have developed a novel biohybrid photocatalyst comprising a light-harvesting protein and a metal-containing catalyst.
22 November 2021
Ultra-high material efficient solar cell using semiconductor nanowires
19 November 2021Laurie Donaldson
Researchers have developed a novel electrochemical method for recovering cobalt and nickel from lithium-ion battery electrodes.
19 November 2021
Researchers have shown that applying short, high-voltage pulses can improve the joining of materials in solid-state batteries.
17 November 2021
A new analysis technique will help scientists create better supercapacitors, especially supercapacitors made from layers of different materials.
16 November 2021
An exploration of the amazing world of surface science.
11 November 2021
By combining copper with cellulose nanofibrils from wood, researchers have developed a flexible ion conductor for solid-state batteries.
5 November 2021
Researchers have discovered why applying pressure to a lithium-metal battery can boost its performance, and determined the optimum pressure.
3 November 2021
Using X-ray light and laser light, a new analytical instrument can probe a perovskite’s crystal structure and optical properties as it is synthesized.
3 November 2021
thermoelectric generators based on cellulose paper and thin layers of non-toxic metals promise a cheap and eco-friendly means of heat recovery
1 November 2021Cordelia Sealy