electrochemical modification of carbon fibers makes polymer composites tougher
27 June 2022Cordelia Sealy
By combining semiconductors with flexible polymers, researchers have created a thermoelectric coating for converting low-grade heat into electrical power.
22 June 2022
Non-toxic semiconductor alternative produces green hydrogen
17 June 2022Laurie Donaldson
Tribologists boost power output by keeping friction low
15 June 2022Laurie Winkless
13 June 2022Laurie Winkless
Scientists have developed efficient photocatalysts for splitting water made from inorganic atomic clusters on titanium oxide supports.
9 June 2022
Researchers have developed an oxysulfide glass electrolyte for use in ambient-temperature solid-state sodium-sulfur batteries.
8 June 2022
light-triggered shape-changing device that could serve as a power source for soft robotics
7 June 2022Cordelia Sealy
Researchers have discovered that the tiny defects that limit the efficiency of perovskite solar cells are also responsible for their degradation over time.