egg white proteins can be transformed into ultralightweight carbon aerogels for highly efficient water purification
28 September 2022Cordelia Sealy
By doping with a high-entropy alloy, researchers have been able to make lithium-ion battery cathodes with nickel rather than cobalt.
28 September 2022
High-quality cathode material made from sodium
22 September 2022Laurie Donaldson
Using selectively doped gallium nitride, researchers have created new high-power electronic devices that are more energy efficient than previous versions.
12 September 2022
Scientists have created a zinc battery that contains a sustainable, biodegradable gel electrolyte made from crab shells.
9 September 2022
Researchers have discovered that stress gradients in a solid electrolyte that affect the passage of ions can lead to the failure of solid-state batteries.
9 September 2022
Researchers have developed copper-based metal oxides that can take part in redox reactions for carbon capture at high temperatures.
8 September 2022
Researchers have developed a low-cost battery that uses aluminum and sulfur as electrode materials, with a molten salt electrolyte in between.
2 September 2022