High-frequency sound waves can remove the rust that inhibits the performance of a novel battery technology based on the 2D material MXene.
Electrode screen-printing process for health monitoring
Italian researchers look to cellulose and carbon for ingestible devices
Improved high-voltage, hermetically sealed microbattery design
A novel nano-coating can protect spacecraft and satellites from harsh solar radiation while also harvesting energy for future use.
Breakthrough in light-driven microelectronic devices
Using saltwater and nanoengineering, researchers have produced a novel aqueous battery that could help prevent electric vehicle fires.
By coating porous electrodes in a light-harvesting material, researchers have developed a device that can produce hydrogen fuel from humidity and sunlight.
A new method of heating and cooling called ‘ionocaloric cooling’ uses the movement of ions to induce a phase change in a mixture of salt and solvent.
A combination of high-powered electron microscopy and computational modeling has revealed what occurs when lithium-ion batteries degrade.