A researcher at Georgia Tech holds a perovskite-based solar cell, which is flexible and lighter than silicon-based versions. Photo: Rob Felt, Georgia Tech.Perovskite-based solar cells are simple and cheap to produce, offer flexibility that could unlock a whole new range of installation methods and places, and in recent years have reached energy efficiencies approaching those of traditional silicon-based cells. But figuring out how to produce perovskite-based energy devices that last longer than a couple of months has been a challenge.
Now researchers from Georgia Institute of Technology, the University of California (UC) San Diego and Massachusetts Institute of Technology have reported new findings about perovskite solar cells that could lead the way to devices that perform better.
"Perovskite solar cells offer a lot of potential advantages because they are extremely lightweight and can be made with flexible plastic substrates," said Juan-Pablo Correa-Baena, an assistant professor in the Georgia Tech School of Materials Science and Engineering. "To be able to compete in the marketplace with silicon-based solar cells, however, they need to be more efficient."
In a paper published in Science, the researchers now report uncovering the mechanisms that lead to improved performance when alkali metal is added to traditional perovskites.
"Perovskites could really change the game in solar," said David Fenning, a professor of nanoengineering at UC San Diego. "They have the potential to reduce costs without giving up performance. But there's still a lot to learn fundamentally about these materials."
To understand perovskite crystals, it's helpful to think of its crystalline structure as a triad. One part of the triad is typically formed from the element lead. The second part is typically made up of an organic component such as methylammonium, and the third part is often comprised of other halides such as bromine and iodine.
In recent years, researchers have focused on testing different recipes to achieve better efficiencies, such as adding iodine and bromine to the lead component of the structure. Later, they tried substituting cesium and rubidium to the part of the perovskite typically occupied by organic molecules.
"We knew from earlier work that adding cesium and rubidium to a mixed bromine and iodine lead perovskite leads to better stability and higher performance," Correa-Baena said. But little was known about why adding those alkali metals improved the performance of the perovskites.
To understand exactly why it seemed to work, the researchers used high-intensity X-ray mapping to examine the perovskites at the nanoscale. "By looking at the composition within the perovskite material, we can see how each individual element plays a role in improving the performance of the device," explained Yanqi (Grace) Luo, a nanoengineering PhD student at UC San Diego.
The researchers discovered that when cesium and rubidium were added to the mixed bromine and iodine lead perovskite, it caused the bromine and iodine to mix together more homogeneously. This resulted in up to 2% higher conversion efficiency than without the additives.
"We found that uniformity in the chemistry and structure is what helps a perovskite solar cell operate at its fullest potential," Fenning said. "Any heterogeneity in that backbone is like a weak link in the chain."
Even so, the researchers also observed that, while adding rubidium or cesium caused the bromine and iodine to become more homogenous, the halide metals themselves remained fairly clustered within their own cations, creating inactive ‘dead zones’ in the solar cell that produce no current.
"This was surprising," Fenning said. "Having these dead zones would typically kill a solar cell. In other materials, they act like black holes that suck in electrons from other regions and never let them go, so you lose current and voltage.
"But in these perovskites, we saw that the dead zones around rubidium and cesium weren't too detrimental to solar cell performance, though there was some current loss. This shows how robust these materials are but also that there's even more opportunity for improvement."
These findings add to the understanding of how the perovskite-based devices work at the nanoscale and could lay the groundwork for future improvements.
"These materials promise to be very cost effective and high performing, which is pretty much what we need to make sure photovoltaic panels are deployed widely," Correa-Baena said. "We want to try to offset issues of climate change, so the idea is to have photovoltaic cells that are as cheap as possible."
This story is adapted from material from Georgia Institute of Technology, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.