These scanning electron microscope images show an anode made of asphalt, graphene nanoribbons and lithium at left and the same material without lithium at right. The material was developed at Rice University and shows promise for high-capacity lithium-metal batteries that charge up to 20 times faster than commercial lithium-ion batteries. Image: Tour Group/Rice University.A touch of asphalt may be the secret to high-capacity lithium-metal batteries that charge 10 to 20 times faster than commercial lithium-ion batteries, according to scientists at Rice University.
The Rice lab of chemist James Tour has developed anodes comprising porous carbon made from asphalt that showed exceptional stability after more than 500 charge-discharge cycles. A high-current density of 20 milliamps per square centimeter showed the material's promise for use in rapid charge and discharge devices that require high-power density. The finding is reported in a paper in ACS Nano.
"The capacity of these batteries is enormous, but what is equally remarkable is that we can bring them from zero charge to full charge in five minutes, rather than the typical two hours or more needed with other batteries," Tour said.
The Tour lab previously used the same derivative of asphalt –untreated gilsonite – to capture greenhouse gases from natural gas. This time, the researchers mixed gilsonite with conductive graphene nanoribbons, before coating the composite with lithium metal through electrochemical deposition.
Finally, they combined the anode with a sulfurized-carbon cathode to make full batteries for testing. These batteries demonstrated a high-power density of 1322 watts per kilogram and high-energy density of 943 watt-hours per kilogram.
Testing also revealed another significant benefit: the carbon mitigated the formation of lithium dendrites. These mossy deposits can invade a battery's electrolyte; if they extend far enough, they short-circuit the anode and cathode, causing the battery to fail, catch fire or explode. But the asphalt-derived carbon prevents any dendrite formation.
An earlier project by the lab found that an anode of graphene and carbon nanotubes also prevented the formation of dendrites. Tour said that this new composite is simpler.
"While the capacity between the former and this new battery is similar, approaching the theoretical limit of lithium metal, the new asphalt-derived carbon can take up more lithium metal per unit area, and it is much simpler and cheaper to make," he said. "There is no chemical vapor deposition step, no e-beam deposition step and no need to grow nanotubes from graphene, so manufacturing is greatly simplified."