An LED light powered by a prototype rechargeable battery that uses the sodium-chlorine chemistry recently developed by researchers at Stanford University. Photo: Guanzhou Zhu.An international team led by researchers at Stanford University has developed a novel rechargeable battery that can store up to six times more charge than current batteries.
This advance, reported in a paper in Nature, brings battery researchers one step closer to creating a high-performance rechargeable battery that can achieve two top goals: allow cell phones to be charged only once a week instead of daily and electric vehicles to travel six times farther without a recharge.
The new so-called alkali metal-chlorine batteries, developed by a team of researchers led by Stanford chemistry professor Hongjie Dai and doctoral candidate Guanzhou Zhu, rely on the back-and-forth chemical conversion of sodium chloride or lithium chloride to chlorine. As proof of concept, the researchers created a working prototype sodium metal-chlorine coin battery.
After electrons travel from one side of a rechargeable battery to the other during use, recharging reverts the chemistry back to its original state to await another use. Non-rechargeable batteries have no such luck. Once drained, their chemistry cannot be restored.
“A rechargeable battery is a bit like a rocking chair. It tips in one direction, but then rocks back when you add electricity,” Dai explained. “What we have here is a high-rocking rocking chair.”
The reason no one had yet created a high-performance rechargeable sodium-chlorine or lithium-chlorine battery is that chlorine is too reactive and challenging to convert back to a chloride with high efficiency. In the few cases where others were able to achieve a certain degree of rechargeability, the battery performance proved poor.
Dai and Zhu did not actually set out to create a rechargeable sodium-chlorine or lithium-chlorine battery at all, but merely to improve their existing battery technologies using thionyl chloride. This chemical is one of the main ingredients of lithium-thionyl chloride batteries, which are a popular type of single-use battery first invented in the 1970s.
But in one of their early experiments involving chlorine and sodium chloride, the Stanford researchers noticed that the conversion of one chemical to another had somehow stabilized, resulting in some rechargeability. “I didn’t think it was possible,” Dai said. “It took us about at least a year to really realize what was going on.”
Over the next several years, the team elucidated the reversible chemistries and sought ways to make them more efficient by experimenting with many different materials for the battery’s positive electrode. The big breakthrough came when they made the electrode using an advanced porous carbon material from collaborators Yuan-Yao Li and Hung-Chun Tai at the National Chung Cheng University of Taiwan. This carbon material has a nanosphere structure filled with many ultra-tiny pores. In practice, these hollow spheres act like a sponge, sopping up copious amounts of otherwise touchy chlorine molecules and storing them for later conversion to salt inside the micropores.
“The chlorine molecule is being trapped and protected in the tiny pores of the carbon nanospheres when the battery is charged,” Zhu explained. “Then, when the battery needs to be drained or discharged, we can discharge the battery and convert chlorine to make NaCl – table salt – and repeat this process over many cycles. We can cycle up to 200 times currently and there’s still room for improvement.”
The result is a step toward the holy grail of battery design – high energy density. The researchers have so far achieved 1200 milliamp hours per gram of positive electrode material, while the capacity of commercial lithium-ion batteries today is up to 200 milliamp hours per gram. “Ours has at least six times higher capacity,” Zhu said.
The researchers envision their batteries one day being used in situations where frequent recharging is not practical or desirable, such as in satellites or remote sensors. Many otherwise usable satellites are now floating in orbit, obsolete due to their dead batteries. Future satellites equipped with long-lived rechargeable batteries could be fitted with solar chargers, extending their usefulness many times over.
For now though, the working prototype they’ve developed might still be suitable for use in small everyday electronics like hearing aids or remote controls. For consumer electronics or electrical vehicles, much more work remains to be done to engineer the battery structure, increase the energy density, scale up the batteries and increase the number of cycles.