To make the new energy-storage material, a thin film is first deposited via a pulsed-laser deposition process in this chamber. The bright ‘plume’ is the laser hitting the target and depositing the film. Photo: Martin/UC Berkeley.Capacitors that rapidly store and release electric energy are key components in modern electronics and power systems. However, the most commonly used capacitors have low energy densities compared with other storage systems, like batteries or fuel cells, which in turn cannot discharge and recharge rapidly without sustaining damage.
Now, as reported in a paper in Science, researchers have managed to achieve the best of both worlds. By introducing isolated defects to a type of commercially available thin film in a straightforward post-processing step, a team led by researchers at the US Department of Energy (DOE)'s Lawrence Berkeley National Laboratory (Berkeley Lab) has demonstrated that a common material can be transformed into a top-performing energy storage material.
This research was supported by the Materials Project, an open-access online database that delivers the largest collection of materials properties to scientists around the globe. Among other goals, the Materials Project combines both computational and experimental efforts to accelerate the design of new functional materials. This includes understanding ways to manipulate known materials in ways that improve their performance.
Growing requirements for cost reduction and device miniaturization have helped to drive the development of high-energy-density capacitors. Capacitors are commonly used in electronic devices to maintain power supply while a battery is being charged. The new material developed at Berkeley Lab could ultimately combine the efficiency, reliability and robustness of capacitors with the energy storage capabilities of larger-scale batteries. Applications include personal electronic devices, wearable technology and car audio systems.
The material is based on a so-called ‘relaxor ferroelectric’, a ceramic that undergoes a rapid mechanical or electronic response to an external electric field. Relaxor ferroelectrics are already used as capacitors in applications like ultrasonics, pressure sensors and voltage generators.
Applying an electric field to a ferroelectric material drives changes in the orientation of its electrons. At the same time, the field also drives a change in the energy stored in the material, making it a good candidate for use beyond a small-scale capacitor. The problem is how to optimize the ferroelectric so that it can be charged to high voltages and discharged very rapidly – billions of times or more – without sustaining damage that would render it unsuitable for long-term use in applications such as computers and vehicles.
Researchers in the lab of Lane Martin, a faculty scientist in the Materials Sciences Division (MSD) at Berkeley Lab and professor of materials science and engineering at the University of California, Berkeley, have now come up with a solution to this problem. This involves introducing local defects that allow the ferroelectric material to withstand bigger voltages.
"You've probably experienced relaxor ferroelectrics on a gas grill. The button that lights the grill operates a spring-loaded hammer that smacks a piezoelectric crystal, which is a type of relaxor, and creates a voltage that ignites the gas," explained Martin. "We've demonstrated that they can also be made into some of the best materials for energy-storage applications as well."
Placing a ferroelectric material between two electrodes and increasing the electric field causes charge to build up. During discharge, the amount of energy available depends on how strongly the material's electrons orient, or become polarized, in response to the electric field. However, most such materials typically cannot withstand a large electric field before the material fails. The fundamental challenge, therefore, is to find a way to increase the maximum possible electric field without sacrificing the polarization.
The researchers turned to an approach that they had previously developed to ‘turn off’ conductivity in a material. By bombarding a thin film with highly charged ions, they were able to introduce isolated defects. These defects trap the material's electrons, preventing their motion and decreasing the film's conductivity by orders of magnitude.
"In ferroelectrics, which are supposed to be insulators, having charge that leaks through them is a major issue. By bombarding ferroelectrics with beams of high-energy ions, we knew we could make them better insulators," said Jieun Kim, a doctoral researcher in Martin's group and lead author of the paper. "We then asked: ‘Could we use this same approach to make a relaxor ferroelectric withstand bigger voltages and electric fields before it catastrophically fails?’"
The answer turned out to be ‘yes’. Kim first fabricated thin films of a prototypical relaxor ferroelectric called lead magnesium niobite-lead titanate. Then he bombarded the films with high-energy helium ions at the Ion-Beam Analysis Facility operated by the Accelerator Technology and Applied Physics (ATAP) Division at Berkeley Lab. The helium ions knocked target ions from their sites to create point defects. Measurements showed that the ion-bombarded film had more than twice the energy storage density of previously reported values and 50% higher efficiencies.
"We were originally expecting the effects to be mostly from reducing the leakage with isolated point defects. However, we realized that the shift in the polarization-electric field relationship due to some of those defects was equally important," said Martin. "This shift means that it takes larger and larger applied voltages to create the maximum change in polarization." The result suggests that ion bombardment can help to overcome the trade-off between being highly polarizable and easily breakable.
The same ion beam approach could improve other dielectric materials for energy storage, while also providing researchers with a tool to repair problems in already-synthesized materials. "It would be great to see folks use these ion-beam approaches to 'heal' materials in devices after the fact if their synthesis or production process didn't go perfectly," said Kim.
This story is adapted from material from Lawrence Berkeley National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.