Arizona State University researchers have created a new compound crystal material that promises to help produce advances in a range of scientific and technological pursuits.
ASU electrical engineering professor Cun-Zheng Ning says the material, called erbium chloride silicate, can be used to develop the next generations of computers, improve the capabilities of the Internet, increase the efficiency of silicon-based photovoltaic cells to convert sunlight into electrical energy, and enhance the quality of solid-state lighting and sensor technology.
The breakthrough involves the first-ever synthesis of a new erbium compound in the form of a single-crystal nanowire, which has superior properties compared to erbium compounds in other forms.
Erbium is one of the most important members of the rare earth family in the periodic table of chemical elements. It emits photons in the wavelength range of 1.5 micrometers, which are used in the optical fibers essential to high-quality performance of the Internet and telephones.
Erbium is used in doping optical fibers to amplify the signal of the Internet and telephones in telecommunications systems. Doping is the term used to describe the process of inserting low concentrations of various elements into other substances as a way to alter the electrical or optical properties of the substances to produce desired results. The elements used in such processes are referred to as dopants.
“Since we could not dope as many erbium atoms in a fiber as we wish, fibers had to be very long to be useful for amplifying an Internet signal. This makes integrating Internet communications and computing on a chip very difficult,” Ning explains.
“With the new erbium compound, 1000 times more erbium atoms are contained in the compound. This means many devices can be integrated into a chip-scale system,” he says. “Thus the new compound materials containing erbium can be integrated with silicon to combine computing and communication functionalities on the same inexpensive silicon platform to increase the speed of computing and Internet operation at the same time.”
Erbium materials can also be used to increase the energy-conversion efficiency of silicon solar cells.
Silicon does not absorb solar radiation with wavelengths longer than 1.1 microns, which results in waste of energy – making solar cells less efficient.
Erbium materials can remedy the situation by converting two or more photons carrying small amounts of energy into one photon that is carrying a larger amount of energy. The single, more powerful photon can then be absorbed by silicon, thus increasing the efficiency of solar cells.
Erbium materials also help absorb ultraviolet light from the sun and convert it into photons carrying small amounts of energy, which can then be more efficiently converted into electricity by silicon cells. This color-conversion function of turning ultraviolet light into other visible colors of light is also important in generating white light for solid-state lighting devices.
While erbium’s importance is well-recognized, producing erbium materials of high quality has been challenging, Ning says.
The standard approach is to introduce erbium as a dopant into various host materials, such as silicon oxide, silicon, and many other crystals and glasses.
What is unique about the new erbium material synthesized by Ning’s group is that erbium is no longer randomly introduced as a dopant. Instead, erbium is part of a uniform compound and the number of erbium atoms is a factor of 1000 more than the maximum amount that can be introduced in other erbium-doped materials.
Increasing the number of erbium atoms provides more optical activity to produce stronger lighting. It also enhances the conversion of different colors of light into white light to produce higher-quality solid-state lighting and enables solar cells to more efficiently convert sunlight in electrical energy.
Like many scientific discoveries, the synthesis of this new erbium material was made somewhat by accident.
“Similar to what other researchers are doing, we were originally trying to dope erbium into silicon nanowires. But the characteristics demonstrated by the material surprised us,” he says. “We got a new material. We did not know what it was, and there was no published document that described it. It took us more than a year to finally realize we got a new single-crystal material no one else had produced.”
Ning and his team are now trying to use the new erbium compound for various applications, such as increasing silicon solar cell efficiency and making miniaturized optical amplifiers for chip-scale photonic systems for computers and high-speed Internet.
“Most importantly,” he says, “there are many things we have yet to learn about what can be achieved with use of the material. Our preliminary studies of its characteristics show it has many amazing properties and superior optical quality. More exciting discoveries are waiting to be made.”
This story is reprinted from material from Arizona State University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.