Molecules in gelatin naturally self-assemble in flat sheets, carrying the metal ions with them (left). Heating the mixture to 600°C burns off the gelatin, leaving nanometer-thin sheets of metal carbide (right). Image: Xining Zang illustration, copyright Wiley.A cheap and effective new catalyst developed by researchers at the University of California (UC), Berkeley, can generate hydrogen fuel from water just as efficiently as platinum, currently the best – but also the most expensive – water-splitting catalyst out there.
The new catalyst, which is composed of nanometer-thin sheets of metal carbide, is manufactured using a self-assembly process that relies on a surprising ingredient: gelatin, the material that gives Jell-O its jiggle.
"Platinum is expensive, so it would be desirable to find other alternative materials to replace it," said senior author Liwei Lin, professor of mechanical engineering at UC Berkeley. "We are actually using something similar to the Jell-O that you can eat as the foundation, and mixing it with some of the abundant earth elements to create an inexpensive new material for important catalytic reactions."
The researchers report the new catalyst in a paper in Advanced Materials.
A zap of electricity can break apart the strong bonds that tie water molecules together, producing oxygen and hydrogen gas, the latter of which is an extremely valuable source of energy for powering hydrogen fuel cells. Hydrogen gas can also be used to help store energy from renewable yet intermittent energy sources like solar and wind power, which produce excess electricity when the sun shines or when the wind blows, but which go dormant on rainy or calm days.
But simply sticking an electrode in a glass of water is an extremely inefficient method of generating hydrogen gas. For the past 20 years, scientists have been searching for catalysts that can speed up this reaction, making it practical for large-scale use.
"The traditional way of using water gas to generate hydrogen still dominates in industry. However, this method produces carbon dioxide as by-product," said first author Xining Zang, who conducted the research as a graduate student in mechanical engineering at UC Berkeley. "Electrocatalytic hydrogen generation is growing in the past decade, following the global demand to lower emissions. Developing a highly efficient and low-cost catalyst for electrohydrolysis will bring profound technical, economical and societal benefit."
To create the catalyst, the researchers followed a recipe nearly as simple as making Jell-O from a box. They mixed gelatin and a metal ion – either molybdenum, tungsten or cobalt – with water, and then let the mixture dry.
"We believe that as gelatin dries, it self-assembles layer by layer," Lin said. "The metal ion is carried by the gelatin, so when the gelatin self-assembles, your metal ion is also arranged into these flat layers, and these flat sheets are what give Jell-O its characteristic mirror-like surface."
Heating the mixture to 600°C triggers the metal ion to react with the carbon atoms in the gelatin, forming large, nanometer-thin sheets of metal carbide. The unreacted gelatin simply burns away.
The researchers tested the efficiency of the catalysts by placing them in water and running an electric current through them. When stacked up against each other, molybdenum carbide proved most efficient at splitting water, followed by tungsten carbide and then cobalt carbide, which didn't form thin layers as well as the other two. Mixing molybdenum ions with a small amount of cobalt boosted the performance even more.
"It is possible that other forms of carbide may provide even better performance," Lin said.
The two-dimensional shape of the catalyst is one of the reasons why it is so successful. That is because the water has to be in contact with the surface of the catalyst to be split into oxygen and hydrogen, and the large surface area of the sheets mean that the metal carbides are extremely efficient for their weight.
Because the recipe is so simple, it could easily be scaled up to produce large quantities of the catalyst, the researchers say.
"We found that the performance is very close to the best catalyst made of platinum and carbon, which is the gold standard in this area," Lin said. "This means that we can replace the very expensive platinum with our material, which is made in a very scalable manufacturing process."