Viewed through the semi-transparent solar cells, the cherries on the tree are clearly visible. The new manufacturing process could produce meter-scale electricity-producing windows. Photo: Xinjing Huang, Optoelectronic Components and Materials Group, University of Michigan.In an important step toward bringing transparent solar cells to home windows, researchers at the University of Michigan (U-M) have developed a way to manufacture their highly efficient and semi-transparent solar cells.
"In principle, we can now scale semi-transparent organic solar cells to 2m by 2m, which brings our windows much closer to reality," said Stephen Forrest, professor of electrical engineering at U-M and corresponding author of a paper on this work in Joule.
Traditional silicon-based solar cells are completely opaque, which works for solar farms and roofs but would defeat the purpose of windows. However, organic solar cells, in which the light absorber is a type of plastic, can be transparent.
Organic solar cells have lagged behind their silicon-based cousins for energy-producing purposes due to engineering challenges such as low solar-to-electricity efficiencies and short lifespans. But recent work in Forrest's lab has achieved record solar-to-electricity efficiencies of 10% and estimated lifetimes of up to 30 years.
So the team has now turned its attention to making these transparent solar cells manufacturable. A significant challenge is creating the micron-scale electrical connections between individual cells that comprise the solar module. Conventional methods that use lasers to pattern the cells can easily damage the organic light absorbers.
Instead, the team developed a multistep peel-off patterning method that achieved micron-scale resolution. They deposited thin films of plastic and patterned them into extremely thin strips. Then, they set down the organic and metal layers. Next, they peeled off the strips, creating very fine electrical interconnections between the cells.
The group connected eight semi-transparent solar cells, each 4cm by 0.4cm and separated by 200µm-wide interconnections, to create a single 13cm2 module. The solar-to-electricity efficiency of 7.3% was approximately 10% less than for the individual solar cells in the module. But this small efficiency loss does not increase with the size of the module, meaning similar efficiencies are expected for meter-scale panels as well.
With a transparency nearing 50% and a greenish tint, the cells are suitable for use in commercial windows. Higher transparencies that are likely preferred for the residential market are easily achieved by this same technology.
"It is now time to get industry involved to turn this technology into affordable applications," said Xinjing Huang, a U-M doctoral student in applied physics and first author of the paper.
Eventually, the flexible solar cell panel will be sandwiched between two windowpanes. The goal for these energy-generating window films is to be about 50% transparent with a solar-to-electricity efficiency of 10–15%. Forrest believes this can be achieved within a couple years.
"The research we are doing is derisking the technology so that manufacturers can make the investments needed to enter large-scale production," Forrest said.
The technique can also be generalized to other organic electronic devices. And in fact, Forrest’s group is already applying it to OLEDs for white lighting.
This story is adapted from material from the University of Michigan, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.