Schematic of an ORFB assembled with a BTMAP-Fc catholyte and a BTMAP-Vi anolyte, incorporating an anion exchange membrane separator. The pH and anion combinations in the supporting electrolyte are detailed below the schematic. The electron and ion flow during charging is depicted by a solid line, and the equivalent flow during the discharge process is depicted by dashed lines. Image: Washington University in St. Louis/Vijay Ramani.The pace of progress in the renewable energy sector is limited not only by the technology for capturing energy from the Sun, wind, oceans or the Earth’s radiant heat, but also by the ability to effectively store and deploy that energy after it has been harnessed.
The primary hurdle in the development of reliable batteries that can be scaled to serve the needs of the grid is, unsurprisingly, cost — of materials, but also of the research necessary to find the best materials.
At Washington University in St. Louis, a research team in the lab of Vijay Ramani, a professor at the McKelvey School of Engineering, has developed a way to determine which materials are best suited for use as a key component in any organic redox flow battery (ORFB) for grid-scale energy storage: the electrolyte. The team reports its work in a paper in the Proceedings of the National Academy of Sciences.
Organic redox flow batteries (ORFBs) are low-cost. Their design makes them cheaper than lithium-ion batteries per unit of electricity stored at scale, and they use inexpensive organic materials for the battery actives (cathode and anode).
“In our system, we are using viologen, which is widely used as a herbicide and is very inexpensive,” said first author Kritika Sharma, a PhD student in Ramani’s lab. “If we are using such organic actives, then the main decision is, ‘What electrolyte do we dissolve it in to maximize battery efficacy?’”
Traditionally, answering that question has involved a lot of trial-and-error experimentation and analyses. What Ramani’s team found, however, has the potential to eliminate much of this work: a universal descriptor that indicates which electrolytes are best paired with organic actives. This universal descriptor is a parameter known as the solvent reorganizational energy.
Ramani’s research team, consisting of Shrihari Sankarasubramanian and Javier Parrondo, in addition to Sharma, looked at two actives (a ferrocene dichloride cathode and a propyl viologen tetrachloride anode) and six electrolytes (sulfuric acid, hydrochloric acid, methane sulfonic acid, sodium sulfate. sodium chloride and sodium methane sulfonate) at neutral and acidic pHs. They found their universal descriptor indicated the combinations with the most complementary chemistry and battery performance characteristics — low discharge polarization and high open-circuit voltage.
“Our descriptor i.e., solvent reorganizational energy, allowed us to show that low pH electrolytes with methane sulfonate or chloride counterions worked best,” said Sankarasubramanian, joint first author of the paper and assistant professor of chemical engineering at the University of Texas at San Antonio. “We were able to predict this with an hour of experimentation in the lab instead of the usual days or weeks.”
Although the paper shows results from a limited number of combinations, Sharma said the descriptor can be generalized, as it is based on the fundamental relationship between the actives and the electrolytes, and correlates the kinetic and transport properties in the system.
With a generalizable method to predict the best electrolytes for a given organic active, the development of new storage technologies will become more efficient — and none too soon.
“Grid-scale energy storage is required to have a stable grid when intermittent solar- and wind-based generators are dominant,” Sharma said. “Our universal descriptor can help speed up the development of new storage solutions.”
This story is adapted from material from the Washington University in St. Louis, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.