The left visual shows that a lithium aluminum titanium phosphate (LATP) pellet that touches lithium metal will be immediately reduced. The severe side reaction between lithium and the solid electrolyte will cause the battery to fail in several cycles. The right visual shows that an artificial boron nitride film is chemically and mechanically robust against lithium. It electronically isolates LATP from lithium, but still provides stable ionic pathways when infiltrated by polyethylene oxide (PEO) and thus allows stable cycling. Image: Qian Cheng/Columbia Engineering.The grand challenge to improve energy storage and enhance battery life, while ensuring safe operation, is becoming ever more critical as batteries are increasingly used to power everything from portable devices to electric vehicles. A team from Columbia Engineering, led by Yuan Yang, assistant professor of materials science and engineering, has now developed a new method for safely prolonging battery life by adding a nano-coating of boron nitride (BN) to stabilize solid electrolytes in lithium metal batteries. The team reports its findings in a paper in Joule.
While conventional lithium ion (Li-ion) batteries are widely used in daily life, they have a low energy density, resulting in a shorter battery life. What is more, because of the highly flammable liquid electrolyte inside them, they can short out and even catch fire.
Energy density could be improved by using lithium metal to replace the graphite anode used in Li-ion batteries: lithium metal's theoretical capacity for the amount of charge it can deliver is almost 10 times higher than that of graphite. But dendrites often form during lithium plating, and if these dendrites penetrate the membrane separator in the middle of the battery, they can create short-circuits, raising concerns about battery safety.
"We decided to focus on solid, ceramic electrolytes. They show great promise in improving both safety and energy density, as compared with conventional, flammable electrolytes in Li-ion batteries," says Yang. "We are particularly interested in rechargeable solid-state lithium batteries because they are promising candidates for next-generation energy storage."
Most solid electrolytes are ceramic, and therefore non-flammable, eliminating safety concerns. In addition, solid ceramic electrolytes have a high mechanical strength that can actually suppress lithium dendrite growth, allowing a lithium metal coating to become an option for the anode. However, most solid electrolytes are unstable against lithium, being easily corroded by lithium metal.
"Lithium metal is indispensable for enhancing energy density and so it's critical that we be able to use it as the anode for solid electrolytes," says Qian Cheng, the paper's lead author and a postdoctoral research scientist working in Yang's group. "To adapt these unstable solid electrolytes for real-life applications, we needed to develop a chemically and mechanically stable interface to protect these solid electrolytes against the lithium anode. It is essential that the interface not only be highly electronically insulating, but also ionically conducting in order to transport lithium ions. Plus, this interface has to be super-thin to avoid lowering the energy density of batteries."
To address these challenges, the team worked with colleagues at Brookhaven National Laboratory and the City University of New York. They deposited a 5–10nm-thick boron nitride (BN) nano-film as a protective layer to isolate the electrical contact between the lithium metal and the ionic conductor (the solid electrolyte), along with a trace quantity of polymer or liquid electrolyte to infiltrate the electrode/electrolyte interface.
They selected BN as a protective layer because it is chemically and mechanically stable with lithium metal, providing a high degree of electronic insulation. They designed this BN layer to have intrinsic defects, through which lithium ions can pass, allowing it to serve as an excellent separator. In addition, BN can be readily prepared by chemical vapor deposition to form large-scale, atomically thin, continuous films.
"While earlier studies used polymeric protection layers as thick as 200μm, our BN protective film, at only 5–10 nm thick, is record-thin – at the limit of such protection layers – without lowering the energy density of batteries," Cheng says. "It's the perfect material to function as a barrier that prevents the invasion of lithium metal to solid electrolyte. Like a bullet-proof vest, we've developed a lithium-metal-proof 'vest' for unstable solid electrolytes and, with that innovation, achieved long cycling lifetime lithium metal batteries."
The researchers are now extending their method to a broad range of unstable solid electrolytes and further optimizing the interface. They expect to fabricate solid-state batteries with high performance and long-cycle lifetimes.
This story is adapted from material from Columbia Engineering, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.