Diagram of an aqueous battery with the novel 3D 'zinc-M alloy' anode and a seawater electrolyte. Image: Zhenxing Feng, Oregon State University. Researchers in the College of Engineering at Oregon State University (OSU) have developed a battery anode based on a new nanostructured alloy that could revolutionize the way energy storage devices are designed and manufactured. The novel zinc- and manganese-based alloy also opens the door to replacing solvents commonly used in battery electrolytes with something much safer and inexpensive, as well as abundant: seawater. The researchers report their work in a paper in Nature Communications .
"The world's energy needs are increasing, but the development of next-generation electrochemical energy storage systems with high energy density and long cycling life remains technically challenging," said Zhenxing Feng, a chemical engineering researcher at OSU. "Aqueous batteries, which use water-based conducting solutions as the electrolytes, are an emerging and much safer alternative to lithium-ion batteries. But the energy density of aqueous systems has been comparatively low, and also the water will react with the lithium, which has further hindered aqueous batteries' widespread use."
A battery stores power in the form of chemical energy and through reactions converts it to the electrical energy needed to power vehicles, cell phones, laptops, and many other devices and machines. A battery consists of two terminals – the anode and cathode, typically made of different materials – as well as a separator and electrolyte, a chemical medium that allows for the flow of electrical charge. In a lithium-ion battery, charge is carried via lithium ions as they move through the electrolyte from the anode to the cathode during discharge, and back again during recharging.
"Electrolytes in lithium-ion batteries are commonly dissolved in organic solvents, which are flammable and often decompose at high operation voltages," Feng said. "Thus, there are obviously safety concerns, including with lithium dendrite growth at the electrode-electrolyte interface; that can cause a short between the electrodes."
Dendrites resemble tiny trees growing inside a lithium-ion battery and can pierce the separator, like thistles growing through cracks in a driveway. The result is unwanted, and sometimes unsafe, chemical reactions that can cause batteries to catch fire.
Aqueous batteries are a promising alternative for safe and scalable energy storage, Feng said. Aqueous electrolytes are cost-competitive, environmentally benign, capable of fast charging and high-power densities, and highly tolerant of mishandling. But their large-scale use has been hindered by a limited output voltage and low energy density (batteries with a higher energy density can store more energy, while batteries with a higher power density can release large amounts of energy more quickly).
Researchers at OSU, the University of Central Florida and the University of Houston have now designed a novel anode made up of a three-dimensional 'zinc-M alloy' (M refers to manganese and other metals), which could prove of use in aqueous batteries.
"The use of the alloy with its special nanostructure not only suppresses dendrite formation by controlling the surface reaction thermodynamics and the reaction kinetics, it also demonstrates super-high stability over thousands of cycles under harsh electrochemical conditions," Feng said. "The use of zinc can transfer twice as many charges than lithium, thus improving the energy density of the battery.
"We also tested our aqueous battery using seawater, instead of high purity deionized water, as the electrolyte," he added. "Our work shows the commercial potential for large-scale manufacturing of these batteries."
Feng and PhD student Maoyu Wang used X-ray absorption spectroscopy and imaging to track the atomic and chemical changes of the anode at different operation stages, which confirmed how the 3D alloy was functioning in the battery.
"Our theoretical and experimental studies proved that the 3D alloy anode has unprecedented interfacial stability, achieved by a favorable diffusion channel of zinc on the alloy surface," Feng said. "The concept demonstrated in this collaborative work is likely to bring a paradigm shift in the design of high-performance alloy anodes for aqueous and non-aqueous batteries, revolutionizing the battery industry."
This story is adapted from material from Oregon State University , with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source .