The new sodium-ion material retains the high energy density of a lithium-ion cathode, but replaces most of the lithium atoms (green) with sodium (yellow). The layered structure of the new material also incorporates manganese (purple) and oxygen (red). Image: University of Texas at Dallas.In the battle of the batteries, lithium-ion technology is the reigning champion, powering everything from cellphones to an increasing number of electric vehicles on the road. But a novel manganese and sodium-ion-based material developed by researchers at The University of Texas at Dallas, in collaboration with researchers at Seoul National University in Korea, might become a challenger, offering a potentially lower-cost, more ecofriendly option to fuel next-generation devices and electric cars.
Battery cost is a substantial issue, said Kyeongjae Cho, professor of materials science and engineering at The University of Texas at Dallas and senior author of a paper describing the new material in Advanced Materials.
As manufacturers – and consumers – push for more electric vehicles (EVs), lithium production may have a hard time keeping up with increasing demand, Cho said. According to a recent report by the International Energy Agency, the global electric car stock surpassed two million vehicles in 2016 after crossing the one million mark in 2015. The report notes that, depending on the policy environment, there is a good chance that the number of electric cars on the roads will range between nine million and 20 million by 2020 and between 40 million and 70 million by 2025.
In terms of cost savings in the EV battery, using sodium would be less expensive because sodium is more abundant, but it has some drawbacks. "Lithium is a more expensive, limited resource that must be mined from just a few areas on the globe," Cho said. "There are no mining issues with sodium – it can be extracted from seawater. Unfortunately, although sodium-ion batteries might be less expensive than those using lithium, sodium tends to provide 20% lower energy density than lithium." The energy density, or energy storage capacity, of a battery determines the run time of a device.
"We used our previous experience and thought about these issues – how can we combine these ideas to come up with something new to solve the problem?" Cho said.
A battery consists of: a positive electrode, or cathode; a negative electrode, or anode; and an electrolyte in between. In a standard lithium-ion battery, the cathode is made of lithium, cobalt, nickel and oxygen, while the anode is made of graphite. When the battery charges, lithium ions move through the electrolyte to the anode and attach to the carbon. During discharge, the lithium ions move back to the cathode and provide electric energy to run devices.
"There was great hope several years ago in using manganese oxide in lithium-ion battery cathodes to increase capacity, but unfortunately that combination becomes unstable," Cho said.
In the design developed by Cho and his colleagues, sodium replaces most of the lithium in the cathode, and manganese is used instead of the more expensive and rarer elements cobalt and nickel. "Our sodium-ion material is more stable, but it still maintains the high energy capacity of lithium," Cho said. "And we believe this is scalable, which is the whole point of our research. We want to make the material in such a way that the process is compatible with commercial mass production."
Based on their knowledge of the physics and chemistry of other experimental materials, the researchers attacked the problem with rational material design. They first ran computer simulations to determine the configuration of atoms that showed the most promise before making and testing the material in the lab.
Cho said his research is not just about coming up with a better battery. How the research was done is just as important and as interesting, he said.
"When Thomas Edison was trying to develop a light bulb, he tried thousands of different materials for the filament to see which ones worked," Cho said. "To solve very important engineering problems in society today, we need to develop lots of new materials – battery materials, pollution control materials and others. Edison was perfecting one item – the light bulb – but we have so many more technological needs. We don't have time to keep trying to accidentally find the solution."
This story is adapted from material from The University of Texas at Dallas, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.