A eutectic solution turns green as it pulls cobalt from a spent lithium-ion cathode. Photo: Jeff Fitlow/Rice University.Researchers at Rice University have come up with a solution to deal with the glut of used lithium-ion batteries left behind by the ever-increasing demand for electric vehicles, cellphones and other electronic devices.
The Rice lab of materials scientist Pulickel Ajayan used an environmentally friendly deep eutectic solvent to extract valuable elements from the metal oxides commonly used as cathodes in lithium-ion batteries. The goal, the researchers said, is to curtail the use of harsh processes for recycling batteries and to keep them out of landfills.
The deep eutectic solvent, made from the commodity products choline chloride and ethylene glycol, was able to extract more than 90% of cobalt from powdered compounds, and a smaller but still significant amount from used batteries.
"Rechargeable battery waste, particularly from lithium-ion batteries, will become an increasingly menacing environmental challenge in the future as the demand for these, through their usage in electric vehicles and other gadgets, increases dramatically," Ajayan said.
"It's important to recover strategic metals like cobalt that are limited in supply and are critical for the performance of these energy-storage devices," he added. "Something to learn from our present situation with plastics is that it is the right time to have a comprehensive strategy for recycling the growing volume of battery waste." The researchers report their work in a paper in Nature Energy.
"This has been attempted before with acids," said Rice graduate student and lead author Kimmai Tran. "They're effective, but they're corrosive and not eco-friendly. As a whole, recycling lithium-ion batteries is typically expensive and a risk to workers."
Alternative recycling processes also have drawbacks, she said. Pyrometallurgy involves crushing and mixing at extreme temperatures, and generates harmful fumes that require scrubbing. Hydrometallurgy requires caustic chemicals, while other ‘green’ solvents that extract metal ions often require additional agents or high-temperature processes to fully capture the ions.
"The nice thing about this deep eutectic solvent is that it can dissolve a wide variety of metal oxides," Tran said. "It's literally made of a chicken feed additive and a common plastic precursor that, when mixed together at room temperature, form a clear, relatively nontoxic solution that has effective solvating properties."
A deep eutectic solvent is a mixture of two or more compounds that freezes at temperatures much lower than each of its precursors. According to Tran, this offers a way to obtain a liquid from a simple combination of solids.
"The large depression of freezing and melting points is due to the hydrogen bonds formed between the different chemicals," Tran explained. "By selecting the right precursors, inexpensive 'green' solvents with interesting properties can be fabricated."
When Tran joined the Rice group, it was already testing a eutectic solution as an electrolyte in next-generation high-temperature supercapacitors. "We tried to use it in metal oxide supercapacitors, and it was dissolving them," said Rice research scientist and co-corresponding author Babu Ganguli. "The color of the solution would change."
The eutectic was pulling ions from the supercapacitor's nickel. "Our team was discussing this and we soon realized we could use what was thought to be a disadvantage for electrolyte as an advantage for dissolving and recycling spent lithium batteries," Ganguli said.
That became Tran's focus, as she tested deep eutectic solvents on metal oxides at different temperatures and time scales. During tests with lithium cobalt oxide powder, the clear solvent yielded a wide spectrum of blue-green colors that indicated the presence of cobalt dissolved within it. At 180°C (356°F), the solvent could extract nearly 90% of lithium ions, and up to 99% of cobalt ions from the powder under certain conditions.
The researchers built small prototype batteries and cycled them 300 times before exposing the electrodes to the same conditions. The solvent proved adept at dissolving the cobalt and lithium, while also separating the metal oxides from other compounds present in the electrode.
They found that cobalt could be recovered from the eutectic solution through precipitation or even electroplating to a steel mesh, with this latter method potentially allowing the deep eutectic solvent to be reused as well.
"We focused on cobalt," said Rice alumnus Marco Rodrigues, now a postdoctoral researcher at Argonne National Laboratory. "From a resource standpoint, it's the most critical part. The battery in your phone will surely have lots of it. Lithium is very valuable too, but cobalt in particular is not only environmentally scarce but also, from a social standpoint, hard to get." He noted that the US Department of Energy is mounting new efforts to advance battery recycling technologies and recently announced a center for Li-ion battery recycling.
"It's likely we won't be able to recycle and replace mining completely," Tran said. "These technologies are relatively new, and there is a lot of optimization that needs to be done, such as exploring other deep eutectic solvents, but we truly believe in the potential for greener ways to do dirty chemistry. Sustainability is in the heart of the work I do and what I want to do for the rest of my career."
This story is adapted from material from Rice University, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.