Ken Brookes reviews the PM2014 Hardmetals Keynote Paper: ‘Corrosion damage in WC/Co cemented
carbides: residual strength assessment and 3D FIB-FESEM tomography characterization.’

This article appeared in the March/April issue of Metal Powder Report.