Michael E Lutheran, vice president of United States Metal Powders Inc (USMP), based in Flemington, New Jersey has been elected president of the Metal Powde
30 October 2009Richard Felton
The online Global Powder Metallurgy Database (GPMD) has added a new section which contains more than 130 full fatigue curves for a number of Fe, Cu and C s