"The Hardide coating has proven it will 'seal and survive', making it suitable for fire safe applications,” said Robin Gillham, business development manager for flow control at Hardide Coatings.

The ball valves can be used in sour hydrocarbon, sand, high pressure and produced water applications in the oil and gas industry as well as power plant, chemical refinery, cryogenic, nuclear and food manufacturing applications.