Sandvik Coromant plans to introduce HP high-precision coolant to its range of CoroTurn 107 cutting units.
Sandvik Coromant plans to introduce HP high-precision coolant to its range of CoroTurn 107 cutting units.

CoroTurn 107 is suitable for external and internal turning of small, long and slender components. It offers harp cutting edges and improved chip control to help ensure a soft cutting action and low cutting forces.

Coolant pressure of up to 200 bar can now be applied gor use with new high-pressure Coromant Capto units (the pressure limit with standard Capto clamping is 80 bar). In combination with high-precision nozzles, the system offers benefits for the operator in that there are fewer problems with long chips.

The system is designed for wet turning operations, especially in HRSA (ISO S) and stainless steel materials (ISO M) and works well in both high-volume and flexible production featuring mixed materials and/or batch sizes. It is suitable for aerospace, automotive, energy and general engineering applications.