Sandvik Coromant has launched a new series of end mills.
Sandvik Coromant has launched a new series of end mills.

 

Sandvik's new range is designed for a variety of applications, component sizes, shapes and materials, thus helping reduce the requirement to change tools for every different operation.
 
The end mills support all applications from roughing to finishing and profiling operations. Their features include reinforcement of the end teeth to avoid premature chipping, cylindrical land width and flat relief for maximum stability .The new coating on the insert grade GC1630 is extremely resistant to wear and is especially suitable for roughing and finishing dry or wet.