This illustration shows a nitrogen dioxide molecule (depicted in red and gold) confined within a nano-size pore of MFM-300(Al), as characterized using neutron scattering at ORNL. Illustration courtesy of Oak Ridge National Laboratory. Artist: Jill Hemman.
This illustration shows a nitrogen dioxide molecule (depicted in red and gold) confined within a nano-size pore of MFM-300(Al), as characterized using neutron scattering at ORNL. Illustration courtesy of Oak Ridge National Laboratory. Artist: Jill Hemman.

Led by scientists at the University of Manchester in the UK, an international team has developed a metal-organic framework (MOF) material that exhibits a selective, fully reversible and repeatable capability to remove nitrogen dioxide gas from the atmosphere in ambient conditions.

This discovery, confirmed by researchers using neutron scattering at the US Department of Energy's Oak Ridge National Laboratory (ORNL), could lead to air filtration technologies that can cost-effectively capture and convert large quantities of targeted gases, including carbon dioxide and other greenhouse gases. By facilitating the long-term sequestration of these gases, the technologies will help to mitigate air pollution and global warming.

Capturing greenhouse and toxic gases from the atmosphere has long been a challenge, because of their relatively low concentrations and the presence of moisture in the air, which can negatively affect separating targeted gas molecules from other gases. Another challenge has been finding a practical way to release a captured gas for long-term sequestration, such as in underground depleted oil reservoirs or saline-filled rock formations. MOFs offer solutions to many of these challenges, which is why they have been the subject of many recent scientific investigations.

As reported in a paper in Nature Materials, the new MOF, denoted as MFM-300(Al), exhibited the first reversible, selective capture of nitrogen dioxide at ambient pressures and temperatures – at low concentrations – in the presence of moisture, sulfur dioxide and carbon dioxide. Despite the highly reactive nature of nitrogen dioxide, the MFM-300(Al) material proved extremely robust, demonstrating the capability to be fully regenerated, or degassed, multiple times without loss of crystallinity or porosity.

"This material is the first example of a metal-organic framework that exhibits a highly selective and fully reversible capability for repeated separation of nitrogen dioxide from the air, even in presence of water," said Sihai Yang, one of the study's lead authors and a lecturer in inorganic chemistry at the University of Manchester's School of Chemistry.

"Other studies of different porous materials often found performance was degraded in subsequent cycles by the nitrogen dioxide, or that the regeneration process was too difficult and costly," added Martin Schröder, another lead author from the University of Manchester.

As part of the research, the scientists used neutron scattering techniques at ORNL to confirm and precisely characterize how MFM-300(Al) captures nitrogen dioxide molecules.

"Neutrons can easily penetrate dense materials and they are sensitive to lighter elements, such as the hydrogen atoms inside the MFM, which enabled us to observe how the nitrogen dioxide molecules are confined within the nano-size pores," explained Timmy Ramirez-Cuesta, a co-author and coordinator for the chemistry and catalysis initiative at ORNL's Neutron Sciences Directorate. "We benefited from the extremely high sensitivity and quantitative data provided by the VISION vibrational spectroscopy instrument on ORNL's 16-B beamline at the Spallation Neutron Source, which uses neutrons instead of photons to probe molecular vibrations."

The ability to directly observe how and where MFM-300(Al) traps nitrogen dioxide is helping the scientists to validate a computer model of the MOF-based gas separation process, which could help identify how to produce and tailor other materials to capture a variety of different gases.

"Computer modeling and simulation played critical roles in interpreting the neutron scattering data by helping us connect subtle changes in the vibrational spectra to interactions between the MFM-300 and trapped molecules," said Yongqiang Cheng, an ORNL neutron scattering scientist and co-author. "Our goal is to integrate the model with experimental techniques to deliver results that are otherwise difficult to achieve."

This story is adapted from material from Oak Ridge National Laboratory, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier. Link to original source.