Coating specialist Covestro LLC has developed a new processing technique called direct coating to make high-gloss piano black.
16 April 2018
The MPIF says that its annual Basic PM short course will return in 2018 and registration is now available.
6 April 2018
Rodney Brennen, VP of PM parts company Metco Industries, has been appointed president of the Powder Metallurgy Parts Association (PMPA).
5 April 2018
Michael Stucky has been appointed president of the Metal Injection Molding Association (MIMA).
5 April 2018
Global Advanced Metals Pty Ltd and LPW Technology (LPW) have joined forces to promote the use of spheroidized tantalum in 3D metal printing.
3 April 2018