Michael E. Lutheran, president of the MPIF, has been named president of Royal Metal Powders, Inc, a company newly formed by American Chemet Corporation, ba

Global catalyst specialist Evonik Industries has acquired the precious metal powder catalysts business of Udaipur, India-based Ravindra Heraeus Pvt Limited

Atlantic Equipment Engineers, a division of Micron Metals, a manufacturer of metal powders and compounds, has launched a new website with improved informat

Umicore’s board of directors has approved various changes to the organisation of the group.

Miba reports that its sales during the first quarter of 2010 were €98.0 million, a 31.9% increase from the same period the previous year, and a 17.4% incre

The Democratic Republic of Congo (DRC) has signed an agreement with global tin organisation ITRI to improve the traceability of tin in the African country

Talks between the United Steelworkers (USW) union and major North American nickel producer Vale Inco that resumed last Friday in a bid to resolve the bitte

Janicki Industries, based in Sedro-Woolley, Washington, USA has built a giant 1600°F/871°C annealing furnace, designed to handle large-scale, high-precisio

Plansee has developed an extremely corrosion-resistant glass-melting electrode made of molybdenum.

Mr Yoshiyasu Iino, President of DIAMET Corporation, has succeeded Mr Yutaka Mizuno, President of Fine Sinter Co Ltd, for a two-year term to May 2012 as Pre

According to tin member association ITRI, tin consumption has recovered strongly in 2010, with China continuing to provide massive support to the tin marke

Hilti Corp has completed its acquisition of India-based Bhukhanvala Diamond Systems Private Ltd.

The president of the European Powder Metallurgy Association has called for the formation of more specialist groups under the umbrella of the organisation a