Cnem will be responsible for sales of the Group's line of carbonyl nickel powders. Jinchuan recently commissioned a new carbonyl facility with a potential annual output of more than 10 million lbs. 

The company makes a range of products including a filamentary powder, Type N06 and a discrete powder, Type N24 for use in powder metallurgy, specialty alloys, battery and fuel cell electrodes, welding rods, conductive paints and gaskets.

Cnem Corporation is a developer of advanced energy and electronic material and is based in Ontario, Canada.