Höganäs’ Environmental Solutions team, based in China, has secured its first commercial order for a Cleanit EC pilot test installation for a wastewater treatment project near Shanghai.

According to the company, Höganäs’ Cleanit-LC and LC+ media was developed for the removal of arsenic (As), copper (Cu), chromium (Cr), lead (Pb), selenium (Se), and other metals and metalloids from drinking water to parts-per-billion (ppb) or non-detect levels.

The pilot system will be shipped directly to the customer’s site and will commence test runs during the fourth quarter this year, Höganäs said.

‘I could not be prouder and happier for Höganäs, our team, and the China team in particular, for emerging from the corona pandemic with this important win,’ says Louis LeBrun, who heads the Environmental Solutions business.

This story uses material from Höganäs, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.