Acrawax C (ethylene bis-stearamide) is a synthetic lubricant and binder used in powder metallurgy (PM) parts compaction.

Lonza said the capital investment strengthens its role as a reliable and sustainable supplier of the material. It also said that the investment will enhance supply and improve customer response times due to the installation of new process controls, equipment upgrades, and automated product packaging.