By Kari Williamson

“The acquisition of TCB allows Plansee to supply coating materials directly to Korean display, electronics and solar companies,” says Bernhard Schretter, President of Plansee High Performance Materials.

TCB Korea specialises in bonding- the soldering of materials onto carrier materials to enable their use in coating plants.