The furnace, which will feature a working area of 1200 x 1200 x 3500 mm, will be equipped with an “all metal” heating chamber and a system of deep vacuum. The length of the vacuum chamber was dictated by the requirement of processing a titanium element of an aircraft wing. SECO\WARWICK's furnace will be made in accordance with the standard AMS2750D class II tooling type A.

The heating chamber has molybdenum and SS insulation and there will be a working vacuum of 1x10-5 mbar.