Maxtech employs 80 people and produces sintered components for automotive engines and transmissions as well as stainless steel components for exhaust applications.

This joint venture between Miba and Maxtech will provide Indian and international car manufacturers and suppliers with high-tech sintered components. Miba will transfer its powder metal technology to Maxtech and will localise the production of components currently imported to India from Europe. The first technology transfer and localisation projects are already underway. Miba will also provide global sales and engineering support for MPSSL’s stainless steel products, which are used in high-performance exhaust systems.
“The cooperation in India expands our global network and provides our customers with Miba’s technology and best possible support through local product development and production,” says Harald Neubert, CEO of the Miba Sinter Group.