Registration is now open for the Powder Metallurgy Post-Sintering Seminar run by the MPIF.

The two-day seminar, which takes place from 22–23 September 2015, will focus on non-material-removing processes and offers an opportunity for PM industry employees to increase their knowledge of recent breakthroughs and developments within the sintering industry, discuss future trends, learn about the latest equipment, and participate in programs led by industrial experts.

This seminar will help gain the essential information needed to improve the properties of final PM parts through better secondary and finishing operations. Program topics currently include oil impregnation, resin impregnation, copper infiltration, steam treatment, case hardening, brazing, welding, and thermal spray coatings, among others.

For more information, click here.

This story is reprinted from material from the MPIF, with editorial changes made by Materials Today. The views expressed in this article do not necessarily represent those of Elsevier.